Its about real liquid gold.
They don't have a link.
But I just got reply I asked about what temperature to fire, so he said 720 Celsius (1328F) and I fired it to 704 Celsius (1299F) so maybe that is the reason
Search found 7 matches
- Thu Jul 23, 2020 3:31 pm
- Forum: Techniques and Tools
- Topic: Ceramic gold luster
- Replies: 8
- Views: 8489
- Thu Jul 23, 2020 7:13 am
- Forum: Techniques and Tools
- Topic: Ceramic gold luster
- Replies: 8
- Views: 8489
Re: Ceramic gold luster
I don't know, it doesn't say on the bottle, I bought it from the pottery SupplyWhat is the brand.
- Tue Jul 21, 2020 2:56 pm
- Forum: Techniques and Tools
- Topic: Ceramic gold luster
- Replies: 8
- Views: 8489
Re: Ceramic gold luster
Thank you. Works fine on glass Needs to be applied very thin, not puddling. Vent the kiln up to 1000 then close. I do all of that but still not good, maybe it's that band I'm using, I didn't had these problems on the glass but this one is the first time I purchased from pottery Supply before I had o...
- Tue Jul 21, 2020 7:27 am
- Forum: Techniques and Tools
- Topic: Ceramic gold luster
- Replies: 8
- Views: 8489
Ceramic gold luster
Hi,
Can I use the ceramic gold luster for fused glass?
I did use it but it has like stain and puddles on the glass.
I fired to 1300F or do I need to fire higher? Thanks
Can I use the ceramic gold luster for fused glass?
I did use it but it has like stain and puddles on the glass.
I fired to 1300F or do I need to fire higher? Thanks
- Tue Aug 05, 2014 5:07 am
- Forum: Jewelry Making
- Topic: Resize sterling silver ring with fused glass cabochons
- Replies: 5
- Views: 33514
Re: Resize sterling silver ring with fused glass cabochons
Thanks Valerie, but I am asking for a costumer that wants the ring so that will not help me (though I already shipped it but for next time)
- Mon Aug 04, 2014 9:17 am
- Forum: Jewelry Making
- Topic: Resize sterling silver ring with fused glass cabochons
- Replies: 5
- Views: 33514
Re: Resize sterling silver ring with fused glass cabochons
Unless you've done it before (and by the questions it seems you might not have), I'd take it to a jeweler and ask them to do it. They have the correct equipment, they can get the size right, and they can do it without damaging the stone. It's not that expensive, and it's much safer. Thank you Cynth...
- Sun Aug 03, 2014 8:08 am
- Forum: Jewelry Making
- Topic: Resize sterling silver ring with fused glass cabochons
- Replies: 5
- Views: 33514
Resize sterling silver ring with fused glass cabochons
Hi, Can I resize a sterling silver ring with fused glass cabochon with out damage the glass? I mean the cabochon is attach with bezel and I meant to cut the ring to resize it and solder the ring while the glass is still on? any one can advice what can be done? Also if you can help lets say my ring i...