rough edges & needles after slumping - what am I doing wrong?

Hi, I've just completed my second ever slump (yay!). The first one was in a small shallow square mould and came out fine. For this second one I've used a shallower mould (http://www.warm-glass.co.uk/extra-small-square-slumper-with-flat-base-mould-9-x-9-x-35cm-p-2979.html?cPath=96_73) with blue trans...
by helenM
Fri Sep 16, 2016 11:38 am
Forum: Newcomer Forum
Topic: Disposing of ground glass
Replies: 10
Views: 19795

Re: Disposing of ground glass

Thank you!
by helenM
Fri Sep 02, 2016 6:06 am
Forum: Newcomer Forum
Topic: Disposing of ground glass
Replies: 10
Views: 19795

Disposing of ground glass

Hi, I've just bought a diamond pad to grind some glass edges before fire polishing (and to learn how to use it - just bought Paul Tarlow's book to help, excellent book) but I was wondering what the best way of disposing the waste glass is. I thought I would do the grinding in water, let it settle th...
by helenM
Sun Aug 21, 2016 10:57 am
Forum: Techniques and Tools
Topic: Tips on using Amour Etch for etching?
Replies: 6
Views: 10505

Re: Tips on using Amour Etch for etching?

Thanks very much all for your feedback and advice. Guess I have a bottle of armour etch I won't be using now:)
by helenM
Sat Aug 20, 2016 5:08 am
Forum: Techniques and Tools
Topic: Tips on using Amour Etch for etching?
Replies: 6
Views: 10505

Tips on using Amour Etch for etching?

Hi, I've seen a few tutorials online about using Armour Etch etching cream for etching dichroic glass (for example Tanya Veit's one on Youtube). I haven't really tried dichroic glass yet but thought maybe I could get an effect with regular bullseye glass. So I marked off the area I wanted unetched (...
by helenM
Wed Jun 08, 2016 1:22 pm
Forum: Business Topics
Topic: New Bullseye Status
Replies: 7
Views: 36992

Re: New Bullseye Status

Oh yes good news! After what happened to Spectrum recently I was worried my new found glass hobby might soon come to an end. No so happy about the price hike though:( It's not a cheap hobby...
by helenM
Mon May 16, 2016 2:56 pm
Forum: Techniques and Tools
Topic: SPECTRUM GLASS CLOSING DOWN
Replies: 29
Views: 92099

Re: SPECTRUM GLASS CLOSING DOWN

Sad to hear they are closing, hope Uburous do take over.
by helenM
Sat Apr 02, 2016 3:43 am
Forum: Kiln Casting
Topic: Glass casting video
Replies: 4
Views: 11574

Re: Glass casting video

Thanks for the video link, it's very interesting to see just what can be done. Like smallbitz I don't have the space to do this but may some day!
by helenM
Sat Apr 02, 2016 3:36 am
Forum: Photos and Stuff
Topic: "Journey" series
Replies: 7
Views: 14469

Re: "Journey" series

Beautiful work!
by helenM
Sat Apr 02, 2016 3:35 am
Forum: Techniques and Tools
Topic: Has anyone used UGC Accents with Bullseye?
Replies: 2
Views: 4619

Re: Has anyone used UGC Accents with Bullseye?

Thanks very much for your advice Brad. I'm excited to give this a go.
by helenM
Fri Apr 01, 2016 2:31 pm
Forum: Art, philosophy, and content
Topic: Self doubt
Replies: 15
Views: 60326

Re: Self doubt

Coming to this post a bit late lol, but Katie I am exactly the same. I think it's natural to have some elements of self doubt and critisicm when you take pride in what you do. I think it's about learning to manage that so it doesn't intrude so much that it stops you from doing anything at all. I wou...
by helenM
Fri Apr 01, 2016 2:13 pm
Forum: Techniques and Tools
Topic: Has anyone used UGC Accents with Bullseye?
Replies: 2
Views: 4619

Has anyone used UGC Accents with Bullseye?

I've been thinking about getting some UGC Accents in gold, bronze or platinum as I'd like some of these mettalic colours in my designs. But the supplier I can get them from doesn't state what glass COE they are compatible with (and haven't replied to my enquiry about it). I use Bullseye glass, so wa...
by helenM
Fri Apr 01, 2016 2:10 pm
Forum: Newcomer Forum
Topic: Cooling small glass pieces - AFAP?
Replies: 7
Views: 14500

Re: Cooling small glass pieces - AFAP?

Thanks very much everyone. I'm a bit nervous to try skipping the steps 3&4 in case pieces crack - but will test it out sometime - you never know till you try:)
by helenM
Mon Mar 28, 2016 3:08 am
Forum: Newcomer Forum
Topic: Cooling small glass pieces - AFAP?
Replies: 7
Views: 14500

Cooling small glass pieces - AFAP?

I've been using the recommended schedule for firing Bullseye glass in a Paragon SC2 kiln (found on the warm glass site uk). This has been working very well for me (reduced the top temp slightly for squarer edges): 1. rate 400F/222C, temp 1250F/677C, hold 30min 2. 600F/333C, 1445F/785C , 10 3. 999F/9...
by helenM
Mon Mar 28, 2016 2:40 am
Forum: Newcomer Forum
Topic: How best to cut 6mm glass?
Replies: 13
Views: 29318

Re: How best to cut 6mm glass?

Thank you very much everyone for your helpful replies:)
by helenM
Sat Mar 26, 2016 9:42 am
Forum: Newcomer Forum
Topic: How best to cut 6mm glass?
Replies: 13
Views: 29318

How best to cut 6mm glass?

I've been toying with the idea of getting a tile saw to cut up 6mm glass into strips - but I've read a couple of places elsewhere that you can cut 3-6mm glass with a normal hand held glass cutter. I have a Toyo pencil grip cutter but I haven't been able to break the glass. I had a 5cm square piece o...
by helenM
Sun Mar 20, 2016 9:38 am
Forum: Newcomer Forum
Topic: Question about tile cutting saws
Replies: 3
Views: 8985

Re: Question about tile cutting saws

Thanks very much for your help Stephen. Not sure I like the idea of getting doused as I was hoping to use it in my craft room:) Still, next step then is to find out the best type of blades to get. At least I know I can get a cutter like this:)
by helenM
Sat Mar 19, 2016 1:40 pm
Forum: Newcomer Forum
Topic: Question about tile cutting saws
Replies: 3
Views: 8985

Question about tile cutting saws

Hello, I'm new to the forums. I've recently starting making fused glass and am loving it! What I would like to do soon is be able to make larger patterned squares and cut them down to smaller pieces. I've been trying to research the best tools for this, but can't really afford an expensive glass cut...