I am fairly new to fusing and have been trying to follow this discussion but alas am totally confused. This colloidal alumina seems like interesting stuff. Can it be used in place of kiln wash? :? I have to admit, I do not know what ridigizer is, but would like to find out more. Have patience with t...
- Mon Jan 12, 2004 4:13 pm
- Forum: Techniques and Tools
- Topic: Can cracked glass be used
- Replies: 1
- Views: 2869
Can cracked glass be used
One of the pieces I fused had some stress fracture cracking. Do I need to refire the piece or can I use the pieces for my pendants. The piece that fractured is 2" x 3" and is still together in 5 pieces. It was fired in my tiny funky old kiln. I have refired simular pieces and they refused ...