Search found 302 matches

by Stephen Richard
Fri Jun 01, 2012 3:57 am
Forum: Business Topics
Topic: TEACHING
Replies: 1
Views: 4901

Re: TEACHING

If you have a profit margin that you are comfortable with on group courses, that is the least you should charge for a 1-1 course. E.g., if you charge 4 people 200 each, one person on the same course should cost 800 or there about. Of course there is less material used so some compensation for that i...
by Stephen Richard
Fri Jun 01, 2012 3:52 am
Forum: Newcomer Forum
Topic: cutting circles
Replies: 14
Views: 17283

Re: cutting circles

Here is another description of cutting out a circle: First, score the circle, making sure that you start and stop the score line at the same point. Turn the glass over onto a piece of corrugated cardboard, or other surface with some give, with the score line face down. With your thumbs, press along ...