Search found 25 matches
- Thu May 01, 2003 3:33 pm
- Forum: Techniques and Tools
- Topic: 1920's Glass question
- Replies: 4
- Views: 4678
Geri: This is not in the way of help for your problem, but a comment. I have found that ultrasonic machines will remove liver of sulpher patinas, and so as a precaution would not use an ultrasonic on anything with a patina. I believe I have read this caution elsewhere also, but cannot remember the s...
- Wed Apr 23, 2003 12:18 am
- Forum: Kiln Casting
- Topic: Casting Newbie - Info/direction please.
- Replies: 6
- Views: 10221
- Thu Apr 03, 2003 2:32 am
- Forum: Techniques and Tools
- Topic: Dichroic Problem
- Replies: 11
- Views: 14539
Kim: Is there a reason why you are doing two separate firings rather than firing once with the clear cap in place? Since these are cabs (translation: very small pieces) my guess you are firing too hot and/or holding too long, particularly on the second firing. My simple cab construstion consists of ...
- Tue Mar 18, 2003 6:02 pm
- Forum: Techniques and Tools
- Topic: Silver Clay and Glass Molds
- Replies: 6
- Views: 9512
Back when there were only two versions of silver metal clay I experimented with PMC (regular) fused inside glass, and some of my results were published in Jewelry Crafts magazine. It can work if the PMC piece is small, thin, and previously fired, although you do run the risk of silver stain on the g...
- Mon Mar 17, 2003 12:34 am
- Forum: Techniques and Tools
- Topic: My hands are killing me.....
- Replies: 22
- Views: 30899
Phil: I feel your pain (OUCH!). The skin on my finger tips splits often, too. I have many times walked around with bandages on all finger tips--and those don't stay on very well either. I've tried it all--triple anti-biotics, Bag Balm, all the cremes. The best PREVENTATIVE I've found has been Euceri...