Search found 302 matches

by Stephen Richard
Sun Dec 21, 2014 9:50 am
Forum: Techniques and Tools
Topic: Glass hanging methods
Replies: 9
Views: 10557

Re: Glass hanging methods

You are mixing metric and imperial here. 2.5 times difference
by Stephen Richard
Wed Dec 10, 2014 7:37 pm
Forum: Techniques and Tools
Topic: Using spectrum cullet for pate de verre
Replies: 21
Views: 26961

Re: Using spectrum cullet for pate de verre

I have never been able to clean my home made powder or fine frit suitably to avoid discolouration
by Stephen Richard
Tue Dec 09, 2014 6:16 pm
Forum: Techniques and Tools
Topic: Odd crack
Replies: 6
Views: 7573

Re: Odd crack

Sounds to me like too rapid heating on the rise. The glass may have softened at edges and strain became too much for the top layer so splitting.
by Stephen Richard
Sun Dec 07, 2014 3:51 pm
Forum: Newcomer Forum
Topic: More help with frit casting mold, please :)
Replies: 7
Views: 11500

Re: More help with frit casting mold, please :)

The raised area in the brown looks like a bubble.
What kind of firing are you using? let us know the ramp speeds, soaks etc. to see if we can help diagnose the issue.
by Stephen Richard
Fri Dec 05, 2014 3:40 pm
Forum: Techniques and Tools
Topic: Using spectrum cullet for pate de verre
Replies: 21
Views: 26961

Re: Using spectrum cullet for pate de verre

A superficial search of Google indicates hydrochloride will not do the same as sulphur
by Stephen Richard
Sun Nov 16, 2014 3:23 pm
Forum: Newcomer Forum
Topic: How do i know if I've applied enough kiln wash?
Replies: 5
Views: 9752

Re: How do i know if I've applied enough kiln wash?

The kiln wash is generically referred to as a separator. The fact that it is a powdery surface gives less possibility of sticking to the glass, unless you go above 720C. I use Bullseye kiln wash that is tinted pink to give a contrast between a white mould or shelf and the separator. I coat my moulds...
by Stephen Richard
Sun Nov 16, 2014 5:54 am
Forum: Techniques and Tools
Topic: Silver Staining
Replies: 9
Views: 9794

Re: Silver Staining

Thinfire does not provide enough absorption of the silver salts to protect the shelf. You need to use 1mm or thicker fibre paper - or whiting, which is cheaper - to protect the shelf.
by Stephen Richard
Sun Nov 16, 2014 5:48 am
Forum: Techniques and Tools
Topic: Texture / kiln carving
Replies: 11
Views: 15493

Re: Texture / kiln carving

Suzette We really do need the firing conditions -which are more than schedule. The lay up, the glass manufacturer and styles, the kind of kiln, the separators, etc. - any of the conditions that you can think of. 788C does not sound high enough for a full fuse. What kind of glass are you using? Kiln ...
by Stephen Richard
Sun Nov 16, 2014 5:32 am
Forum: Techniques and Tools
Topic: Wall elements
Replies: 3
Views: 5060

Re: Wall elements

On the contrary, heating from the top provides a more even heat to the glass. Heat from the sides heats the edge of the glass first. Because glass is such a poor transmitter of heat, this difference is important. Side heat will get the edges of the glass hotter than the center, sometimes enough to c...
by Stephen Richard
Wed Nov 12, 2014 6:18 pm
Forum: Newcomer Forum
Topic: Are Bullseye Videos Lessons worth the expense?
Replies: 18
Views: 30482

Re: Are Bullseye Videos Lessons worth the expense?

Peter,
I think they aim for one a month
Stephen
by Stephen Richard
Sat Nov 08, 2014 6:01 am
Forum: Techniques and Tools
Topic: Thermocouple
Replies: 17
Views: 18796

Re: Thermocouple

I suggest you contact Olympic for guidance
by Stephen Richard
Wed Nov 05, 2014 2:58 am
Forum: Newcomer Forum
Topic: Fusing in small kiln with side elements
Replies: 6
Views: 10295

Re: Fusing in small kiln with side elements

I have a Paragon Fire Fly kiln. It has side elements only. From my reading it appears that a side element kiln should be ramped slower than a top element kiln, is this correct? Yes This kiln is brick lined and very small so it retains a lot of heat. Is there anything about this configuration I shou...
by Stephen Richard
Wed Nov 05, 2014 2:48 am
Forum: Techniques and Tools
Topic: wattage rating
Replies: 3
Views: 4842

Re: wattage rating

Thyere should be a plate with manufacturer's information including voltage and wattage information. It is most likely on side or back, sometimes on the controller, if it is integral to the kiln.
by Stephen Richard
Tue Nov 04, 2014 7:44 pm
Forum: Newcomer Forum
Topic: Are Bullseye Videos Lessons worth the expense?
Replies: 18
Views: 30482

Re: Are Bullseye Videos Lessons worth the expense?

I think they are worth every penny. They are quality productions with assurance the techniques have been thoroughly tested. None of the YouTube variability in quality or the self promotion.
by Stephen Richard
Tue Nov 04, 2014 7:38 pm
Forum: Newcomer Forum
Topic: 4 Seasons.... Break
Replies: 12
Views: 16272

Re: 4 Seasons.... Break

Jan, Essentially you have no anneal cool at all. 530-438 should take about two hours for this tack fusing. 438-370 about one hr. And 370-40 about one hr. (Although it will take much longer for the kiln to cool than the hour. Others may have other ideas, but you should review Bullseye's chart on anne...
by Stephen Richard
Sun Nov 02, 2014 4:56 am
Forum: Techniques and Tools
Topic: Need some kiln recommendations...
Replies: 10
Views: 12225

Re: Need some kiln recommendations...

Bullseye do a nice Paragon based kiln for the 1,000 mark
by Stephen Richard
Fri Oct 17, 2014 3:45 am
Forum: Newcomer Forum
Topic: Why is this cracking?
Replies: 21
Views: 25669

Re: Why is this cracking?

I agree with Bert, and think Rosanna's advice should be followed to determine if the glasses are compatible
by Stephen Richard
Fri Oct 17, 2014 3:40 am
Forum: Techniques and Tools
Topic: fastest - but safe - annealing for float 2 layers
Replies: 22
Views: 23248

Re: fastest - but safe - annealing for float 2 layers

I understood the items to be clear, so ther is no difficulty in using polarised light filters at right angle orientations to see what stress there is. I'm not a fan of the freezer or dishwasher tests, although I understand they work. If the piece is going to be opaque, then, yes, I would make a clea...
by Stephen Richard
Thu Oct 16, 2014 3:52 am
Forum: Techniques and Tools
Topic: fastest - but safe - annealing for float 2 layers
Replies: 22
Views: 23248

Re: fastest - but safe - annealing for float 2 layers

Throughout this discussion on "how fast is safe" there has been no mention of stress testing at the end of the process. That will tell you if the annealing was sufficient. If there is significant stress, slow the annealing down.
by Stephen Richard
Wed Aug 20, 2014 3:34 am
Forum: Newcomer Forum
Topic: Fusing Three Layers
Replies: 7
Views: 14757

Re: Fusing Three Layers

The shelf should be below the temperature sensor. The side elements should be baffled so radiant heat does not directly affect the edges of the piece (avoiding the risk of sealing the edges too early) For this kind of lay up I would use something like (all in Celsius) 200-625, 10mins 50-675,30 mins ...