Search found 716 matches
- Tue Jul 15, 2014 1:55 pm
- Forum: Kiln Casting
- Topic: Refractory Materials
- Replies: 4
- Views: 8874
Re: Refractory Materials
Ask on craftweb hot glass. They will know.
- Sun Jun 22, 2014 3:56 pm
- Forum: Techniques and Tools
- Topic: New Fiber Kiln Prefiring
- Replies: 11
- Views: 10888
Re: New Fiber Kiln Prefiring
In my kilns I need less heat to get the same results in my fiber kiln than in my bricj kiln. Adjust your schedules.
- Sat Jun 21, 2014 1:13 pm
- Forum: Techniques and Tools
- Topic: New Fiber Kiln Prefiring
- Replies: 11
- Views: 10888
Re: New Fiber Kiln Prefiring
Just fire it at 9999 up to top temp and hold for 15 OR so min. Leave out a peephole plug or vent in some other fashion throughout. The firing.
- Wed Jun 11, 2014 9:26 am
- Forum: Techniques and Tools
- Topic: glass breaking
- Replies: 3
- Views: 5324
Re: glass breaking
check to see if your thermocouple has degraded. your temps could be off. r.
- Sat Jun 07, 2014 8:01 am
- Forum: Techniques and Tools
- Topic: Textured Molds by Creative Paradise
- Replies: 10
- Views: 14910
Re: Textured Molds by Creative Paradise
do like dana says. fuse your blank on a kiln shelf then texture with that mold. r.
- Tue May 27, 2014 6:03 pm
- Forum: Techniques and Tools
- Topic: 1/16 fiber paper
- Replies: 6
- Views: 9333
Re: 1/16 fiber paper
you can smooth rough feeling paper by sprinkleing with dry kw or alumina hydrate and rubbing that around with your hand or a dry paint brush.
- Thu May 22, 2014 8:59 am
- Forum: Business Topics
- Topic: Customers Asking for Discounts
- Replies: 19
- Views: 30743
Re: Customers Asking for Discounts
heh. had a couple come in to the kdh co op the otherday while i was doing my desk shift. he was pushy and wanted to know just what sort of discounts we offered. i said none. did not say sorry or anything other than 'none'. well that flummoxed him as he had some sort of further schpiel prepared that ...
- Thu May 22, 2014 8:22 am
- Forum: Photos and Stuff
- Topic: Mistakes and Taking Risks
- Replies: 46
- Views: 61140
Re: Mistakes and Taking Risks
lemonade
- Thu May 22, 2014 8:20 am
- Forum: Business Topics
- Topic: Customers Asking for Discounts
- Replies: 19
- Views: 30743
Re: Customers Asking for Discounts
i always just say ' no. i can not under cut my galleries. ' period. on the other hand i usually sort of give a piece away at each show. usually to a young person who is obviously yearning for a piece but does not have the cash and does not ask for a discount. i will sell for half just to make both o...
- Thu May 22, 2014 8:08 am
- Forum: Techniques and Tools
- Topic: Devitrification in New Kiln/Kiln Shelf
- Replies: 8
- Views: 9666
Re: Devitrification in New Kiln/Kiln Shelf
and vent throughout that firing.
- Thu May 22, 2014 8:06 am
- Forum: Techniques and Tools
- Topic: Fusing glass to animal skull
- Replies: 9
- Views: 10843
Re: Fusing glass to animal skull
darn. now i am hungry.
- Sat May 17, 2014 8:02 am
- Forum: Kiln Casting
- Topic: fusing youghegheny
- Replies: 9
- Views: 14386
Re: fusing youghegheny
Too thin. Glass wants to be 1/4" thick at full fuse
I am assuming you are using float glass.
I am assuming you are using float glass.
- Fri May 16, 2014 8:23 am
- Forum: Photos and Stuff
- Topic: Blackbird
- Replies: 17
- Views: 23487
Re: Blackbird
awsome! i can hear that bird.
- Fri May 16, 2014 8:20 am
- Forum: Techniques and Tools
- Topic: Glass Painting & Firing Questions
- Replies: 35
- Views: 52985
Re: Glass Painting & Firing Questions
the tin side of float will resist paint more than the air side.
- Thu May 15, 2014 3:11 pm
- Forum: Techniques and Tools
- Topic: Dang bubbles
- Replies: 13
- Views: 16333
Re: Dang bubbles
i like a hold at 1100f as well. things just go better over all if i spend 20 or so min there.
- Thu May 15, 2014 8:19 am
- Forum: Techniques and Tools
- Topic: Dang bubbles
- Replies: 13
- Views: 16333
Re: Dang bubbles
A single 3mm piece of glass, or was it two 3mm sheets for 6mm total? If one sheet, that's the problem. Other than that, was the kiln shelf with kiln wash dry? If not, bubbles. Do you have a picture of the bubbles? That will help a lot, too. Change the 300 DPH to 1425 to AFAP to 1425. No reason to g...
- Wed May 14, 2014 2:55 pm
- Forum: Techniques and Tools
- Topic: Silver fuming
- Replies: 4
- Views: 6133
Re: Silver fuming
i wonder if the silver will get back into the kiln atmosphere if a firing after the fuming is hotter? i know that if i use my kiln to burn off labels that i have to fire it empty a few hundred deg higher to clean it or i will have horrible devit on the next firing. by horrible i mean crystalline wit...
- Sun May 04, 2014 9:42 am
- Forum: Business Topics
- Topic: Donations/Pricing
- Replies: 14
- Views: 22440
Re: Donations/Pricing
here is a good essay on donating art. http://www.huffingtonpost.com/mat-gleason/charity-art-auctions-_b_872953.html i donate only to local causes like raising money directly for someone in a bad way or empty bowls . i do not donate to top heavy national organizations such as komen. https://www.faceb...
- Thu Apr 17, 2014 9:05 pm
- Forum: Techniques and Tools
- Topic: Old, and I mean really old kiln wash?
- Replies: 3
- Views: 5193
Re: Old, and I mean really old kiln wash?
wash a piece of tile and fuse on that and see what happens. r.
- Mon Mar 24, 2014 9:47 am
- Forum: Techniques and Tools
- Topic: Gold leaf quality
- Replies: 3
- Views: 5462
Re: Gold leaf quality
gold LEAF generally dissapears into the glass. gold FOIL is what you want for fusing. rosanna