Patti S

new moldmaking material

Post by Patti S »

http://www.glasscolor.com/catalog/casti ... otInst.asp

OCR has it on sale right now. The product sheet says it can be used for multiple firings, especially if kilnwashed. Has anyone tried this stuff yet?
Colin & Helen

Post by Colin & Helen »

No not as yet.. it sounds like the best thin since sliced bread.. I bet it won't be sold in my neck of the woods..Colin
Carolyn Ledbetter
Posts: 17
Joined: Mon Mar 10, 2003 1:29 pm
Location: Venice, Florida

Post by Carolyn Ledbetter »

Sounds interesting! Hope someone tries it out and posts their results. I've not had much sucess with damp mold materials. They were hard to work with and very stinky!
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

It sounds like a new, and even more expensive, variation of HydraPerm, available through U.S. Gypsum.