Flower pot melting debit at top temperature
Posted: Fri Jul 07, 2017 2:10 am
Hi all!
Is there a a prescription of how much glass would flow from an aperture of a certain size for a given time and temperature?
I'm about to cast 8 to 10kg (17 to 22 pounds) of S96 glass from a flower pot into a mould with a core. Because of the core, I will close the stock hole in the center and cut 2 new apertures - round cornered rectangulars, about 1x2cm each. Any predictions of how much time it will take at 840C/1550F?
My kiln is very big and I [u][b]cannot[/b][/u] open it while firing.
Thanks!
Is there a a prescription of how much glass would flow from an aperture of a certain size for a given time and temperature?
I'm about to cast 8 to 10kg (17 to 22 pounds) of S96 glass from a flower pot into a mould with a core. Because of the core, I will close the stock hole in the center and cut 2 new apertures - round cornered rectangulars, about 1x2cm each. Any predictions of how much time it will take at 840C/1550F?
My kiln is very big and I [u][b]cannot[/b][/u] open it while firing.
Thanks!