Top temperature for Ferro Sunshine enamels

Posted: Wed Oct 11, 2023 2:41 pm
by Maggie Abdel Rahman
Hello!
If you have used Ferro Sunshine enamels ...

what is the temperature required for the enamels to just ADHERE to glass?
the enamels will be applied to one sheet of float glass in a first firing.
I would aporeciate your recommendations

Re: Top temperature for Ferro Sunshine enamels

Posted: Wed Oct 11, 2023 2:48 pm
by Brad Walker
We fire to just adhere to 1325F.

Note that some colors will not mature to final color at this temperature.

You can also add Mixing Flux to lower the temperature.

Re: Top temperature for Ferro Sunshine enamels

Posted: Wed Oct 11, 2023 5:06 pm
by Maggie Abdel Rahman
Thank you