Glass fever,
I am fusing the 2 sheets of glass and draping at the same time. I will now fuse first then drape. Thank you for your interest- Bill Harrell
by wharrel
Sun Apr 20, 2014 8:36 am
Forum: Newcomer Forum
Topic: Devit on draped bowls
Replies: 7
Views: 24468

Re: Devit on draped bowls

Morgancia--- I am draping 2ea 1/8 in Spectrum glass coe unk. The 2 pieces are 6 in. squares offset 90 degrees which make 8 triangle peaks. I glue tiny bits of glass in four places on the sheets to provide a path for air to evacuate. The glue is Elmer's clear.The outside of the peaks is where most of...
by wharrel
Sun Apr 20, 2014 8:23 am
Forum: Newcomer Forum
Topic: Devit on draped bowls
Replies: 7
Views: 24468

Re: Devit on draped bowls

Jestersbaubles-- I spray Bullseye kiln wash when mold is about 500 degrees. I also put 1 sheet of shelf paper and run the kiln to 1000 before I take the vent out. I drape 2 ea 1/8 inch spectrum glass with elmer's glue to hold them together so they have to fuse tack together, but bubbles are not that...
by wharrel
Sat Apr 19, 2014 4:08 pm
Forum: Newcomer Forum
Topic: Devit on draped bowls
Replies: 7
Views: 24468

Devit on draped bowls

I have draped some bowls on stainless steel molds. Some of the bowls have patches of devitrification. I tried to put homemade devitrification fluid on them and then fire polish them at 1115 for 10 minutes. The bowl slumped a little out of shape but the devit was still there. At 1115 I thought there ...
by wharrel
Mon Feb 17, 2014 4:02 pm
Forum: Newcomer Forum
Topic: drapeing 9in. single sheet over SS bowl
Replies: 12
Views: 38479

Re: drapeing 9in. single sheet over SS bowl

Morganica, no problem, there is no way to determine gender from a name. Thanks for all of the help. Bill Harrell
by wharrel
Sat Feb 15, 2014 11:57 am
Forum: Newcomer Forum
Topic: drapeing 9in. single sheet over SS bowl
Replies: 12
Views: 38479

Re: drapeing 9in. single sheet over SS bowl

Thanks to all for advice. I now have 2 nice bowls, green iridescent and most of the iridescent is on the inside of the bowls and is very pretty. The SS mold seems to have stopped turning black so I am trying a third bowl with no shelf paper. Thanks again-Bill Harrell
by wharrel
Thu Feb 13, 2014 4:21 pm
Forum: Newcomer Forum
Topic: drapeing 9in. single sheet over SS bowl
Replies: 12
Views: 38479

Re: drapeing 9in. single sheet over SS bowl

With all of the good advice I received, I have made 2 bowls by drapeing. The glass is no longer breaking. I do have 2 small problems, the SS pot I am using causes black splotches on the glass and I can't remove them. For the second bowl I used a sheet of kiln shelf paper and reduced the SS to one sm...
by wharrel
Sat Feb 08, 2014 11:20 am
Forum: Newcomer Forum
Topic: drapeing 9in. single sheet over SS bowl
Replies: 12
Views: 38479

Re: drapeing 9in. single sheet over SS bowl

I forgot to state that I had put a 1/32 fiber sheet on top of the SS because I thought the SS was heating up faster than the glass and causing a hotspot where the glass touched the SS. Thanks to all for the help. I will take out the kiln posts and shelves and ramp at 150 up to 1250, hold 30(when slu...
by wharrel
Fri Feb 07, 2014 3:45 pm
Forum: Newcomer Forum
Topic: drapeing 9in. single sheet over SS bowl
Replies: 12
Views: 38479

drapeing 9in. single sheet over SS bowl

I am trying to learn how to drape over a SS bowl with a single 1/8 in glass 9 in in diameter. I am using a paragon 7 kiln. program is as follows 200 1150 10 200 1220 0 400 1240 0 400 1270 20 full 950 90 200 700 10 full 100 0 The circle sheet broke in half about 1000, the second time I tried it, it b...
by wharrel
Fri Nov 22, 2013 11:08 am
Forum: Photos and Stuff
Topic: wind chimes that don't chime, they clunk
Replies: 6
Views: 19702

Re: wind chimes that don't chime, they clunk

I have a picture of the different sizes of glass that will chime and those that will not. I cannot post it here. If you want to see photo email wharrel@cox.net
by wharrel
Thu Nov 21, 2013 1:10 pm
Forum: Photos and Stuff
Topic: wind chimes that don't chime, they clunk
Replies: 6
Views: 19702

Re: wind chimes that don't chime, they clunk

Thanks for your help. I filled my kiln with different sizes of 2 layer glass. Long and slender works whereas short and wide sorta clunks. I made some open rectangles that are wide but the actual sides of the rectangle are about 3/8 inch and they chime nicely. I am gonna slump over a long narrow base...
by wharrel
Tue Nov 19, 2013 1:18 pm
Forum: Photos and Stuff
Topic: wind chimes that don't chime, they clunk
Replies: 6
Views: 19702

Re: wind chimes that don't chime, they clunk

Wow thanks Mike that is a lot of information. Never expected that strong a response.
by wharrel
Mon Nov 18, 2013 4:15 pm
Forum: Photos and Stuff
Topic: wind chimes that don't chime, they clunk
Replies: 6
Views: 19702

wind chimes that don't chime, they clunk

I am new to fusing and I have made some 2 layer chimes. Some chime (nice clear tone when struck) and some don't. Is there a set of rules for this or is there a fool proof way to make the chimes chime. Thanks