Search found 3 matches
- Thu Dec 11, 2003 9:44 am
- Forum: Techniques and Tools
- Topic: air bubbles are they there for good?
- Replies: 3
- Views: 8786
air bubbles are they there for good?
Once you fire a two layer plate and have air bubbles can you fuse it longer to flatten them out or will they bust and leave holes in the piece?[/img]
- Wed Jul 09, 2003 3:36 pm
- Forum: Techniques and Tools
- Topic: edge to edge fusing
- Replies: 3
- Views: 7413
- Wed Jul 09, 2003 10:09 am
- Forum: Techniques and Tools
- Topic: edge to edge fusing
- Replies: 3
- Views: 7413
edge to edge fusing
Just wondering when you do edge to edge fusing if you need a solid bottom piece or can you have 2 layers of the same size pieces on top of each other. If you can what can you do so they do not pull apart? Any help would be appreciated. Jabeb[/b]