Super Spray
I purchased a bottle of "Super Spray" by FuseMaster. I also purchased a small spray bottle. The Super Spray is so thick it wrecked the spray bottle and froze it up the works before anything came out. What did I do wrong? What do the rest of you use to "Spray" "Super Spray&qu...
- Fri Sep 05, 2003 2:38 pm
- Forum: Business Topics
- Topic: selling suggestion
- Replies: 19
- Views: 21219
- Mon Aug 25, 2003 9:59 am
- Forum: Techniques and Tools
- Topic: pot melt help needed
- Replies: 15
- Views: 17678
- Sun Aug 10, 2003 3:35 pm
- Forum: Techniques and Tools
- Topic: My first pot melt.....HELP!
- Replies: 16
- Views: 17983
I just did my first Potmelt after reading all of your comments. I ramped at full speed (since I didn't care if the glass cracked in the pot) up to 1600. The glass started pooping out the standard non-enlarged hole at 1500. At 1600 I soaked for an hour. About 1/2 the glas had come out, so I did anoth...
- Thu Aug 07, 2003 3:03 pm
- Forum: Techniques and Tools
- Topic: Business Card Question
- Replies: 4
- Views: 5285
- Thu Jul 24, 2003 10:09 am
- Forum: Techniques and Tools
- Topic: borax over irid
- Replies: 5
- Views: 6016
- Wed Jul 23, 2003 2:42 pm
- Forum: Techniques and Tools
- Topic: borax over irid
- Replies: 5
- Views: 6016
Borax over Irid
I coated a piece of Green Irid last night before slumping at 1300. No body was there to tell me not to. Turned out nice and shiney, especially the edge.