Sticking stacked glass.
I slump float glass over stainless steel molds. Hi-Temp 1800 works great on the mold. When I slump 2 pieces of glass stacked, I spray a light coat of Hi Temp 1800 on one of them but it leaves a haze that is difficult to remove. Any suggestions to keep the glass from sticking to each other ? Thanks M...