Search found 3 matches
- Sun Nov 02, 2014 7:40 am
- Forum: Newcomer Forum
- Topic: spiky and slightly cloudy ... Help
- Replies: 8
- Views: 23277
Re: spiky and slightly cloudy ... Help
Great info thank you so much ... I have the kiln running as I type so am excited to see the results !
- Wed Oct 29, 2014 11:54 pm
- Forum: Newcomer Forum
- Topic: spiky and slightly cloudy ... Help
- Replies: 8
- Views: 23277
Re: spiky and slightly cloudy ... Help
I'm using Spectrum System 96 Glass. I cleaned it well with 70% iso alcohol before using scent free hair spray as glue.
- Tue Oct 28, 2014 9:15 pm
- Forum: Newcomer Forum
- Topic: spiky and slightly cloudy ... Help
- Replies: 8
- Views: 23277
spiky and slightly cloudy ... Help
Hi, I'm a noobie at this wonderful fusing lark .... I will start from the beginning ... I have a large Skutt ceramic kiln and have managed a great first full fuse just using the center shelf away from the sides and only one shelf not layered as I do with ceramics .... I used thin fire paper and ever...