Re: casting program

Hi thanks for your reply. The Fremont glass was from the same sheet-a beautiful multi color with some gold pink in it. It also did devitrify a bit. As for the hold at 250F I can't explain it-it was the preprogrammed casting program that came with my kiln-the mold is ceramic. I also meant 3.5" w...
by Pam Morgan
Sun May 04, 2014 9:38 am
Forum: Newcomer Forum
Topic: casting program
Replies: 3
Views: 10190

casting program

Hi all! I am a newcomer to hot glass. I've been a stained glass artist for years and have done glass painting, and some minor fusing and slumping. I bought a switchplate cover mold and decided to run it with the factory set casting program on my Hot Start Pro (since I don't really know anything abou...