steaming wax from silica-plaster mold
I'm relatively new to casting glass, am investing a wax positive into a silica-plaster, open-face mold. I'm trying to steam the wax from the mold, have two steamers I've been using. One is a wallpaper steamer, the other a big pot of water on a hefty Bayou Classic propane burner. Both of my steamers ...