Search found 5 matches
- Fri Oct 24, 2014 4:05 pm
- Forum: Newcomer Forum
- Topic: Big bubbles
- Replies: 1
- Views: 7651
Big bubbles
I am such a newbie (read dummy). I have just learned the hard way to keep only the glass I need to use around me when I'm cleaning a piece to get it ready to fire. I put together a 12" plate (very ambitious project) with a solid round on the bottom two concentric rings cut from other glass (I w...
- Sat Aug 23, 2014 9:07 pm
- Forum: Newcomer Forum
- Topic: Fusing Three Layers
- Replies: 7
- Views: 26635
Re: Fusing Three Layers
Another axiom which I am trying to follow myself is (paraphrased), 'more is learned from failure than success.' I also believe this to be true. I'm looking for the confidence to jump off the "fusing glass bridge", I don't want to make mistakes that will jeopardize my kiln (I've heard some...
- Thu Aug 21, 2014 10:47 am
- Forum: Newcomer Forum
- Topic: Fusing Three Layers
- Replies: 7
- Views: 26635
Re: Fusing Three Layers
I will reign myself in and start out with a simple two layer design. I must learn to crawl before I run, lol.
I have so much to learn about this process and I really appreciate all the feedback.
I have so much to learn about this process and I really appreciate all the feedback.
- Wed Aug 20, 2014 10:20 am
- Forum: Newcomer Forum
- Topic: Fusing Three Layers
- Replies: 7
- Views: 26635
Re: Fusing Three Layers
Thanks for the help. I will give this a go.
I have so much to learn and I hate learning the hard way so the advise is most welcome!
I have so much to learn and I hate learning the hard way so the advise is most welcome!
- Mon Aug 18, 2014 1:16 pm
- Forum: Newcomer Forum
- Topic: Fusing Three Layers
- Replies: 7
- Views: 26635
Fusing Three Layers
I am a potter bitten by the hot glass bug! I am just beginning to experiment with the glass kiln option on my Paragon Janus-27 kiln. It is 20" deep so I know I will have to raise the shelf up pretty high. What would be the optimal distance between the glass piece and the elements in the lid? Se...