Search found 5 matches
- Sat Nov 05, 2016 6:53 pm
- Forum: Techniques and Tools
- Topic: cracked in half
- Replies: 9
- Views: 15170
Re: cracked in half
Thanks Valerie. You are right - it is pretty much 90 degrees. Next time I will anneal 4X the usual time. I'm on to other projects for now but when I'm not so sad about it I will give that design another try.
- Thu Nov 03, 2016 2:44 pm
- Forum: Techniques and Tools
- Topic: cracked in half
- Replies: 9
- Views: 15170
Re: cracked in half
Sorry I guess that I didn't make it clear. What you first understood was correct. It is 1 layer of clear with 1 layer of the opal desigh. There were just a few of the small opal pieces that were prefused and are 2 layers. I really appreciate your suggestions with the schedule and next time I will an...
- Wed Nov 02, 2016 6:53 pm
- Forum: Techniques and Tools
- Topic: cracked in half
- Replies: 9
- Views: 15170
Re: cracked in half
It is grippy shelf liner on top of a lazy susan sort of thing that spins around. Do you think that might be a problem? The piece does extend beyond the edges of the spinning thing. The bottom glass is a single layer and most of the pieces on top are 1 layer and a couple of the very small elements ar...
- Tue Nov 01, 2016 9:23 pm
- Forum: Techniques and Tools
- Topic: cracked in half
- Replies: 9
- Views: 15170
Re: cracked in half
Thanks Warren for the suggestion - it is 1 layer of clear with 1 layer of the opal glass. Some of the elements were prefired and a couple of very small elements are 2 layers
- Tue Nov 01, 2016 5:34 pm
- Forum: Techniques and Tools
- Topic: cracked in half
- Replies: 9
- Views: 15170
cracked in half
This piece cracked in half 1 day after coming out of the kiln. It is a mosaic piece made with Spectrum that I tack fused and was in the process of filling in the gaps with frit when I noticed that it had cracked in half. This has only happened to me once before and it was with a piece that was extre...