Search found 1 match

by LAVA Lady
Mon May 11, 2015 11:25 pm
Forum: Techniques and Tools
Topic: Problem slumping into large round molds
Replies: 1
Views: 2879

Problem slumping into large round molds

Hi there, I am hoping someone can offer some advice with this and how I might be able to fix it. It is a problem I have had a couple of times and this time I am beside myself  I am using spectrum 96 glass, I have slumped a piece into a large 500mm round mold. The piece has a full fused base, which ...