Search found 4 matches

by cmcdonald
Tue Jul 07, 2015 3:25 pm
Forum: Techniques and Tools
Topic: Second fuse??
Replies: 4
Views: 9036

Re: Second fuse??

The order of the photos is first white with irid; then blac on Tekta, then blac with clear irid; and last is the white on Tekta. Both pieces using irid are irid up and the dichroic is also up, I.e., them coatings do not face each other. The roughness is only on the dichroic tops and not all of them ...
by cmcdonald
Tue Jul 07, 2015 10:56 am
Forum: Techniques and Tools
Topic: Second fuse??
Replies: 4
Views: 9036

Last Photo

This is the last of the four photos from the previous fusing question post.
Thanks!
by cmcdonald
Tue Jul 07, 2015 10:55 am
Forum: Techniques and Tools
Topic: Second fuse??
Replies: 4
Views: 9036

Second fuse??

I am quite new to the fused glass art world. So with that background, I would like to ask a few questions. I wanted to explore a bit using dichroic, both cut pieces and Bullseye Sizzle Stix. I made four trays, approximately 5 x 9. One is Opaque White on a Tekta base, another is Stiff Black on a Tekt...
by cmcdonald
Mon Jun 22, 2015 10:08 am
Forum: Techniques and Tools
Topic: Best deals on Paragon kilns?
Replies: 7
Views: 20565

Re: Best deals on Paragon kilns?

I purchased at Paragon Pearl 22 in January this year. Bob Paterson (GlassMakerTX@gmail.com) helped me to decide what to get based on the work I wished to do and then he worked with Paragon to have the kiln and a special stand configured etc. for me. He is very informed about all things glass!! Plus ...