Search found 3 matches
- Thu Aug 27, 2015 5:26 pm
- Forum: Techniques and Tools
- Topic: Replacing top elements in Paragon GL 24ATDS
- Replies: 2
- Views: 7060
Re: Replacing top elements in Paragon GL 24ATDS
We can help you find a solution. We would be glad to quote just elements, just the lid, or both. If you give us a pattern we can make a grooved HD ceramic fiber board lid that you can lay your elements into. We also provide a fiberboard slurry glue you then pack into the channel to hold the elements...
- Mon Aug 17, 2015 4:15 pm
- Forum: Newcomer Forum
- Topic: repairing kiln shelf
- Replies: 6
- Views: 22523
Re: repairing kiln shelf
You will be hard pressed to make a good repair. You can cast a new shelf using a Castable 3000 cement. It is good option for making fixtures if you don't mind a rougher surface. A good reminder to bake out moisture slowly after having your kiln in hibernation for a while.
- Thu Aug 06, 2015 4:26 pm
- Forum: Newcomer Forum
- Topic: graphite
- Replies: 4
- Views: 16559
Re: graphite
I agree with the hobbyist. If you are not careful to manage the dust you can and will short out your bushings on your electric motors as the dust is a conductor.