Wed Aug 10, 2016 1:49 pm
Forum: Newcomer Forum
Topic: Straight lines
Replies: 5
Views: 19865

Re: Straight lines

Thank you Doug-your advice works fine when the glass used is opalescent however when it's a clear/transparent mix, the wavy lines are visible from the viewing side. I've seen many artists that use a clear/transparent mix and have no wavy lines on what becomes the bottom of the piece but is initially...
by Michael Mattei
Tue Aug 09, 2016 4:59 pm
Forum: Newcomer Forum
Topic: Straight lines
Replies: 5
Views: 19865

Straight lines

I've had kilns for many years and used them to cast glass that I used for my bevel work in my leaded windows. Just recently I've been fusing work for plate and bowls and am really enjoying it. Naturally I've been viewing other work and am especially taken with strips of color and clear glass fused t...