Hi
I am new to the forum and I am seeking help to solve a problem I am having with kiln casting. On several occasions I have had a very frosty rough surface on the glass where it was in contact with the investment mould. Looks and feels like sandpaper.
Not sure what is happening
Thanks Gaele