Search found 2 matches

by DPEARSON
Thu Aug 06, 2020 3:47 pm
Forum: Techniques and Tools
Topic: Paragon A-66B Glass Firing Schedule
Replies: 3
Views: 7420

Re: Paragon A-66B Glass Firing Schedule

Thanks, Brad. I slumped the wine bottles successfully using a 016 cone. Seems like I can get a selection of cones & just experiment. Is a quick cool-down (by venting the lid) required? For the bottles I just let the kiln cool on its own overnight. You're right, the kiln is very old; my mother pu...
by DPEARSON
Thu Aug 06, 2020 3:20 pm
Forum: Techniques and Tools
Topic: Paragon A-66B Glass Firing Schedule
Replies: 3
Views: 7420

Paragon A-66B Glass Firing Schedule

I have a Paragon A-66B kiln, which I would like to use for fusing glass. The kiln has a kiln-sitter (for use with pyrometric cones) but is not programmable. There is one kiln switch which can be set to Low, Med or High. Other "controls" are a lid which can be vented and 2 peephole plugs wh...