- Thu Aug 06, 2020 3:47 pm
- Forum: Techniques and Tools
- Topic: Paragon A-66B Glass Firing Schedule
- Replies: 3
- Views: 4085
Re: Paragon A-66B Glass Firing Schedule
Thanks, Brad. I slumped the wine bottles successfully using a 016 cone. Seems like I can get a selection of cones & just experiment. Is a quick cool-down (by venting the lid) required? For the bottles I just let the kiln cool on its own overnight. You're right, the kiln is very old; my mother pu...
- Thu Aug 06, 2020 3:20 pm
- Forum: Techniques and Tools
- Topic: Paragon A-66B Glass Firing Schedule
- Replies: 3
- Views: 4085
Paragon A-66B Glass Firing Schedule
I have a Paragon A-66B kiln, which I would like to use for fusing glass. The kiln has a kiln-sitter (for use with pyrometric cones) but is not programmable. There is one kiln switch which can be set to Low, Med or High. Other "controls" are a lid which can be vented and 2 peephole plugs wh...