Grinding
Had to grind small spot after full fusing. Do I need to fire polish the dull spot before slumping or will the slump firing take care of it
- Thu Nov 11, 2021 10:54 am
- Forum: Techniques and Tools
- Topic: Fusing problem
- Replies: 2
- Views: 22136
Fusing problem
Tried tack fusing with Olympic kiln. Did not contour much. Is that a temp problem or hold problem. Did 1000 to 1340 and then full. Am just getting back into fusing.