Search found 2 matches

by Riverglass
Thu Aug 14, 2003 4:59 pm
Forum: Techniques and Tools
Topic: Shelf Primer and Bubbles
Replies: 17
Views: 35266

For what it's worth - this problem had me tearing out my hair for multiple loads of glass! I pre-dried the kiln washed shelf in the kiln to 1000; I air dried it in the house; I bought a new shelf from B Eye. I live in a damp climate near a river and thought the shelf must be absorbing an incredible ...
by Riverglass
Thu Aug 14, 2003 4:52 pm
Forum: Techniques and Tools
Topic: slumping failure. Why????
Replies: 2
Views: 5614

slumping failure. Why????

I was making a mask out of Bullseye. Fused too layers of glass with assorted decorative pieces on top. Fused nicely, annealed for 30 minutes. Used Paragon kiln. When I went to slump it over a wall sconce mold I had purchased at BEye, it cracked in two at approximately 340 degrees. I was slumping at ...