Medium kiln vs Extra-large kiln
I have a medium sized kiln and have contour fused many things in it successfully. Recently, a friend with an extra-large kiln contour fused some items using the exact same schedule that I have had much success with in my medium kiln. The items came out of her kiln with a tack fuse and a few were not...