fusing shattered tempered glass pieces Q

I doubt this is an original idea (although my searches have not found similar info) and would appreciate any tips from those who have tried this! I want to use pieces of shattered tempered glass (safety glass?) to make pieces about 12-15" in diameter that I will then drop slump. I have done som...
by Nancy Conrad
Thu Oct 30, 2003 11:12 am
Forum: Techniques and Tools
Topic: mason stain & carbonates/dioxides question
Replies: 6
Views: 12368

much thanks, Liam, Rosanna, Brian, Gale & Tom

now back to the studio to experiment with more information

this board & those of you answering are awesome--thanks so much to all who make it happen
by Nancy Conrad
Mon Oct 27, 2003 9:57 am
Forum: Techniques and Tools
Topic: mason stain & carbonates/dioxides question
Replies: 6
Views: 12368

mason stain & carbonates/dioxides question

I have a clay background & have some mason stains & carbonates & dioxides all used for colorants in mixing ceramic glazes. Has anyone been successful in using any of these ingredients as colorants in fused glass? What amount have you tried with what results? I am planning on sprinkling t...