removing stickiness

I'm fairly new to fusing, so if this suggestion isn't feasible, please let me know.--When I need to remove adhesive stickers, etc. from most glass and other surfaces I lightly coat the stickers with cooking oil, let it sit a few minutes and the scrape the sticky off. Then I clean as usual. I haven't...