I have slumped soda glass with success twice in 2 greenware molds that I recently purchased. On the 2nd firing one deveoped a hairline crack and on the 3rd firing the other developed a crack. The molds are not the same size and both were bisque fired to 1100C at 100C per hour.
thanks
Kerin
Search found 2 matches
- Sat Oct 18, 2003 5:51 am
- Forum: Techniques and Tools
- Topic: Greenware mold
- Replies: 2
- Views: 5263
- Sun Sep 28, 2003 2:47 am
- Forum: Techniques and Tools
- Topic: Cracked/broken glass during Firing
- Replies: 3
- Views: 7077
Cracked/broken glass during Firing
I am fairly new to glass fusing/slumping. I have had a few successful firnings until today. The pieces on the lower shelf were found to be broken when I opened the kiln. Both were Bullseye on fibre board and beween 2/3 layere thick. One piece had been tack fused previously and the other had been fus...