Search found 5 matches

by SONYA
Mon Apr 19, 2004 6:48 pm
Forum: Techniques and Tools
Topic: Using Sterling Silver wire
Replies: 2
Views: 10256

Using Sterling Silver wire

I've been told that there is a type of Sterling Silver wire which does not go black in the kiln. Is this the case? and if so is it available in Britain?
by SONYA
Mon Apr 19, 2004 6:40 pm
Forum: Techniques and Tools
Topic: Fusing glue
Replies: 15
Views: 48457

Fusing glue

Thanks alot everyone. This is my first time using the Bulletin Board and I'm so impressed with the response. Dan you say you use Super Glue. Do you use this to stick glass together prior to fusing?
by SONYA
Mon Apr 19, 2004 12:52 pm
Forum: Techniques and Tools
Topic: Fusing glue
Replies: 15
Views: 48457

fusing glue

Thank you so much Brad Walker for your reply. I'll now be able be go out and buy some. I imagine it will be cheaper than buying dedicated fusers glue.
by SONYA
Mon Apr 19, 2004 10:34 am
Forum: Techniques and Tools
Topic: Fusing glue
Replies: 15
Views: 48457

fusing glue

I don't think you can get Elmers glue in Scotland(UK) so can anyone in Britain help me out with fusing glue?
by SONYA
Mon Apr 19, 2004 9:46 am
Forum: Techniques and Tools
Topic: Fusing glue
Replies: 15
Views: 48457

Fusing glue

I'm interested in information about fusing glue. Must you always use specially formulated fusing glue or are there other products or normal household things you can use which would just as effective?