Search found 3 matches

by TerriG
Tue Jan 27, 2004 6:23 pm
Forum: Techniques and Tools
Topic: Use of PMC3 and effects on kiln
Replies: 7
Views: 14674

I have fired multiple times with PMC over the last year in my glass kiln with no after affects. You can see the outline of the piece on the shelf after the firing but that hasn't not caused any issues as yet with subsequent glass firings.
by TerriG
Tue Jan 27, 2004 6:09 pm
Forum: Techniques and Tools
Topic: Dichroic on clear
Replies: 6
Views: 14350

I always use layers when firing dichro. If I want depth, I put 1 or more layers of clear (compatible, of course) on top. I also may use a couple of layers of dichro within the piece. Many times these turn out amazing! I've had a couple of the light pattern dichro fade when firing but for the most pa...
by TerriG
Tue Nov 18, 2003 12:19 am
Forum: Techniques and Tools
Topic: Taurus 3 - Inquiring minds want to know...
Replies: 14
Views: 27118

I've had the new Taurus ring saw for a couple of weeks. I really like it. It seems to have more power and is somewhat quieter. I have been using the separating blade on my Taurus 2. I plan to keep my Taurus 2 with the separating blade and use the new Taurus for regular cutting. This way I won't have...