Search found 2 matches

by mcowdery
Fri Jan 30, 2004 7:02 pm
Forum: Techniques and Tools
Topic: Xerography question
Replies: 2
Views: 7711

Xerography question

:?: Help! I read the article Wallace Venable wrote about using laser waterslide decal paper to include a photographic image into a fused glass piece,and I tried to use this method. I got the laser decal paper from Micro Mark and using a toner based copier to copy a black and white image onto the pap...
by mcowdery
Sat Jan 10, 2004 4:54 pm
Forum: Techniques and Tools
Topic: xerography questions
Replies: 6
Views: 16882

xerography questions

I recently read a message from Wallace Venable on using laser waterslide decal paper for the purpose of including a photographic image onto fused glass. I plan to try this, but does anyone know if the inkjet waterslide paper will work as well? I understand that you copy an image onto the shiny side ...