Search found 716 matches
- Mon Jan 13, 2014 5:20 pm
- Forum: Techniques and Tools
- Topic: Failing Silicone: another option?
- Replies: 2
- Views: 4444
Re: Failing Silicone: another option?
ah. good idea. thanks. e 6000 works well for me
- Wed Jan 08, 2014 2:56 pm
- Forum: Photos and Stuff
- Topic: Jelly Fish Lamp
- Replies: 7
- Views: 11186
Re: Jelly Fish Lamp
way cool! where did you get the lamp base? r.
- Wed Jan 08, 2014 8:27 am
- Forum: Techniques and Tools
- Topic: kiln in unheated garage
- Replies: 9
- Views: 11921
Re: kiln in unheated garage
I just read on craftweb that a digitry controller does not like to work if its thermocouple is too cold.
- Tue Jan 07, 2014 12:29 pm
- Forum: Photos and Stuff
- Topic: Indecision
- Replies: 7
- Views: 11765
Re: Indecision
oh yea i can see that that sucks. just send it to mee and it will never bother you again. r.freight collect will be fine.....
- Sat Jan 04, 2014 8:55 am
- Forum: Newcomer Forum
- Topic: New
- Replies: 12
- Views: 14981
Re: New
You can use a kiln for both glass and ceramics with no problems. R.
- Thu Jan 02, 2014 10:10 am
- Forum: Techniques and Tools
- Topic: kiln in unheated garage
- Replies: 9
- Views: 11921
Re: kiln in unheated garage
your controller might get cranky. i put a space heater near mine untill the kiln heats up enough to keep it warm. hmmm. gonna get cold here as well. must check pump house.r.
- Sun Dec 29, 2013 3:03 pm
- Forum: Techniques and Tools
- Topic: Primer Pulling Away from Shelf
- Replies: 5
- Views: 6752
Re: Primer Pulling Away from Shelf
I make my own wash. 8/2 alumina/ kaolin plus some cmc for green strength. Super easy to scrape off. I use 1/1 for molds.
- Sat Dec 28, 2013 2:21 am
- Forum: Techniques and Tools
- Topic: Primer Pulling Away from Shelf
- Replies: 5
- Views: 6752
Re: Primer Pulling Away from Shelf
Put a fresh coat or two of wash between firings. No need to prefire kiln wash.
- Thu Dec 26, 2013 8:16 am
- Forum: Newcomer Forum
- Topic: Shelf wash or paper?
- Replies: 8
- Views: 11717
Re: Shelf wash or paper?
you also need to kilnwash the shelf even if you use the paper. paper can fail if you have a hi temp misfire.
- Tue Dec 17, 2013 10:47 am
- Forum: Techniques and Tools
- Topic: Devit Problem with BE
- Replies: 21
- Views: 32367
Re: Devit Problem with BE
i would lower your first hold to 1100f or a little less. or put in another step with a hold there. your first hold is high enough for the glass to be soft enough grabbing thinfire smutch before it has a chance to get out of the kiln. maybe prop the lid a quarter inch at first. or just use kiln wash.
- Thu Dec 12, 2013 10:56 am
- Forum: Newcomer Forum
- Topic: firing a new mold
- Replies: 9
- Views: 12036
Re: firing a new mold
huh. if the mold has been bisque fired. (those have) then it has been fired to above 1472. i can see no reason why doing like they said would do anything to the ceramic 'interior structures' or whatever. i just see no science behind that statement. cynthia m, you got a clue i am missing? r.
- Wed Dec 11, 2013 9:36 pm
- Forum: Newcomer Forum
- Topic: firing a new mold
- Replies: 9
- Views: 12036
Re: firing a new mold
What manufacturer recommends That? It makes no sense to me. R.
- Wed Dec 11, 2013 9:27 am
- Forum: Newcomer Forum
- Topic: firing a new mold
- Replies: 9
- Views: 12036
Re: firing a new mold
need more info. are you firing green ceramics? if not i see no need to prefire. just kilnwash and use. r.
- Sun Dec 08, 2013 5:45 pm
- Forum: Techniques and Tools
- Topic: Flash kiln burner design?
- Replies: 8
- Views: 11083
Re: Flash kiln burner design?
http://talk.craftweb.com/forumdisplay.php?s=&forumid=4 you might want to ask these guys. rosanna
- Sat Nov 30, 2013 7:12 am
- Forum: Photos and Stuff
- Topic: Damascus, Arizona
- Replies: 17
- Views: 23336
- Sun Nov 24, 2013 9:01 pm
- Forum: Techniques and Tools
- Topic: Hydrogen Sulfide from kiln wash
- Replies: 11
- Views: 10574
Re: Hydrogen Sulfide from kiln wash
well there is organic stuff in whatever binder they use and whatever the chinese haik brush contributed, i do know that my epk/alumina hydrate /cmc mix will go rotten eggy. i used to use a low grade of gum arabic as a binder in kw. whew! toe cheese bugs in that binder. r.
- Sun Nov 24, 2013 7:45 am
- Forum: Techniques and Tools
- Topic: Hydrogen Sulfide from kiln wash
- Replies: 11
- Views: 10574
Re: Hydrogen Sulfide from kiln wash
Damnable Kevin. Now I have to clean coffee of my keyboard. Ha.Kevin Midgley wrote:You didn't leave it long enough.
it is supposed to turn green and slimy.
Just what did you expect to happen?
- Mon Nov 18, 2013 10:46 am
- Forum: Techniques and Tools
- Topic: Kiln wash won't stick to new ceramic mold
- Replies: 5
- Views: 6950
Re: Kiln wash won't stick to new ceramic mold
i would fire it to 1000f or just put it in with whatever firing you do next. if that does not help then what you have is a result of how the mold was poured. the clay can be compressed in an area and less able to easily hold kw.
- Tue Nov 12, 2013 8:38 am
- Forum: Techniques and Tools
- Topic: Removing glass plug from diamond drill bit
- Replies: 25
- Views: 33458
Re: Removing glass plug from diamond drill bit
bead mandril pushed out from behind after every hole.pita. next time i have a bunch of holes to drill i am going to line up a helper. i will use 3 or 4 drill bits and the helper will be poking out the plugs while i drill. r.
- Wed Oct 30, 2013 8:44 am
- Forum: Techniques and Tools
- Topic: Using partially cracked glass in layered piece
- Replies: 4
- Views: 5687
Re: Using partially cracked glass in layered piece
every time i use a cracked piece the crack shows.