Search found 41 matches

by camaro
Wed Apr 14, 2004 6:06 pm
Forum: Techniques and Tools
Topic: Bullseye sample sets- Striking Colors
Replies: 9
Views: 21077

Striking color

I just ordered from BE and it does show the before and after strike color in their new catalog. Unfortunately you are correct, yes you will need to fire the glass at fuse temp to get the strike color. I also WAS going to order some of them, but like you I did not want to keep samples of the strike c...
by camaro
Fri Mar 26, 2004 5:44 pm
Forum: Techniques and Tools
Topic: full fuse problem
Replies: 1
Views: 2938

full fuse problem

I have a jen ken oval 13", I just tried the following: RA 400 F 1450 Hold 15 min. off I am using Spectrum 96, my problem is on some pieces the center has thinned alot, and on another I have two extra large bubbles in the piece, what did I do wrong? Also I checked in the peep hole at 1398 is whe...
by camaro
Sun Mar 21, 2004 9:01 pm
Forum: Photos and Stuff
Topic: Critic's Corner (temp) Jim's Flagstones
Replies: 10
Views: 14210

critique

Personally I like them both, but what the hay I'll try to critique. First of all to me they look like ceramic glazes. Where the beige is it appears to be a stippled or sponged effect. However I could be wrong. I would say the bowl was the second project. Bowl: I like the movement, in which the cente...
by camaro
Sun Mar 21, 2004 8:44 pm
Forum: Techniques and Tools
Topic: Criticism
Replies: 65
Views: 83731

critique

After reading everyones post, I am curious--It seems that alot of people on this board seem to know each other personally from attending various events, or classes. For someone like me, that would love to attend such events and participate in various classes or shows, however will probably never be ...
by camaro
Fri Mar 19, 2004 5:32 pm
Forum: Techniques and Tools
Topic: Drilling finished dichroic pieces?
Replies: 18
Views: 21162

drilling dichro

Well I hate to admit it, but I use a plastic basin filled with enough water to cover a 1" X 2" piece of board. I then use my handy dremel with a standard diamond tip bought from the local home depot, works for me. Just buy a few extra they do dull in a short time, or maybe its me? Anyway I...
by camaro
Fri Mar 19, 2004 12:23 pm
Forum: Techniques and Tools
Topic: Respirator ?
Replies: 4
Views: 5991

Respirator ?

Questions: Can I vacum out my kiln?
What type of repirator do I need- please be specific.
Can I purchase one from Home Depot--Lowes?

Will I damage the existing Kiln wash already on my kiln shelves or kiln floor?

Thank you
camaro :?
by camaro
Thu Mar 18, 2004 7:03 pm
Forum: Photos and Stuff
Topic: Havin' fun with pot melts
Replies: 23
Views: 40525

potmelts

WOW !!!!
Those are extrodinary, absolutely beautiful. I wish I knew the the technique, if you'd like to share I'd love to try one my self. I have a large kiln that could handle it.
Excellent job.
camaro
by camaro
Mon Mar 15, 2004 1:10 pm
Forum: Techniques and Tools
Topic: calendar
Replies: 7
Views: 9302

calendar

What exactly does it offer? photos of other glass artisans and bios from this glass site, pros, semi-pro begginers ? glass art photos? Is this the first one ever made?
thanks
camaro
by camaro
Mon Mar 08, 2004 12:17 pm
Forum: Techniques and Tools
Topic: crushing glass for frits
Replies: 13
Views: 19699

I use a coffee grinder, I cut glass into small pieces and insert push button and try to control the size of frit I need by the amount of pusing the button. It makes great pulvarized frit for painting, as well as med. of large frit pieces. I bought my coffee grinder at the local Walmart, cheap. Howev...
by camaro
Sun Feb 22, 2004 6:40 pm
Forum: Techniques and Tools
Topic: Stringer Storage
Replies: 16
Views: 29325

Stringers

Just a thought, I use clear tubing with plasic chair end caps, you can get the clear tubing various diameters. They work for me.
camaro
by camaro
Fri Feb 13, 2004 7:30 pm
Forum: Techniques and Tools
Topic: Jen-Ken Kiln question
Replies: 12
Views: 13154

I have a Jen Ken and it has a viewing window, its great. I can watch it, but remember to get a # 5 shade welding glasses, you could burn your retinas, at least thats what I've been told. Also Marty at Centre DeVerre is great for any questions you may have, extremely helpful. Marty if you read this T...
by camaro
Sun Feb 08, 2004 11:28 am
Forum: Techniques and Tools
Topic: Wall art bracket hanging ?
Replies: 2
Views: 4110

Wall art bracket hanging ?

Is there a way that a plate/ Bowl can be made to hang. If so after it is fused and then slumped how can I keep the right side shiny, while trying to fuse something on the back of the piece. If I use fiber paper won't that cause a roughness on the front? Any advice greatly appreciated. Thanks in adva...
by camaro
Tue Jan 06, 2004 8:37 pm
Forum: Kiln Casting
Topic: mould making for novice = 0 responses ?
Replies: 4
Views: 6564

mould making for novice = 0 responses ?

As of 1/6/04 I see that there have been 53 lookers yet no one has responded. I realize its a pain in the @*!!! to help newbies, but give me a break!!!!!!!
camaro

I'm learning alot from this board, most are very friendly and helpful and others are guarding their GOLD.

Thanks for nothing.
by camaro
Mon Jan 05, 2004 2:51 pm
Forum: Kiln Casting
Topic: mold making for novice
Replies: 5
Views: 8445

mold making for novice

I have 2 books one by Boyce Lundstrom and the Warm Glass however the instructions are for those who already maybe know the basics of mold making. Where can I find specifics on mold making step by step, for casting, and 2 part mold making? I've read alot on this board, and alot of people use a variet...
by camaro
Sun Jan 04, 2004 11:51 pm
Forum: Business Topics
Topic: How to get a copywrite
Replies: 5
Views: 6913

copyright info

Yes it is true, anything that is created and tangible is auto copyrighted, however, I am an artist in a variety of mediums, and if you have several drawings that you would like to protect for any future publishing then, gather them up, list each individual drawing, name each and submit to money I be...
by camaro
Sun Dec 07, 2003 12:00 pm
Forum: Techniques and Tools
Topic: Glass or paint?
Replies: 0
Views: 7096

Glass or paint?

I just came back from a trip, I saw something in glass that was awesome. I will only descripe a piece because it was so complicated and gorgeous and would be a novel if I truly explain all the details. On this Fused glass there were clear thick solid medium( about 4") round disks. On these disk...
by camaro
Sat Nov 15, 2003 8:09 pm
Forum: Techniques and Tools
Topic: Thank you to Cliff Swanson
Replies: 1
Views: 3363

Thank you to Cliff Swanson

Clff I will try and see what I've done tomorrw regarding programing the RTC 1000. You have been so kind and generous I hope I can do you proud !! If you have an email, please post in private message to me, I could use a friend with this type of controller, because I would like to have a way to ask d...
by camaro
Fri Nov 14, 2003 9:09 pm
Forum: Techniques and Tools
Topic: RTC 1000 controller confusion!
Replies: 3
Views: 7082

RTC 1000 controller confusion!

I just bought a large kiln, however I know 0 about programing, Marty at Centre DeVerre has been extremely helpful. Yet I can't continue to make long distance cell calls, my family does need to eat. I do have it programed like this: Tack Fusing or Slumping (single layer slumping) User 4 segment 1 ra ...
by camaro
Wed Nov 12, 2003 12:07 pm
Forum: Techniques and Tools
Topic: Atten: Jewelry Pendant artist
Replies: 17
Views: 18591

Atten: Jewelry Pendant artist

I have asked before, and what I am looking for is: A flat or round disc with a cylinder at the top, that a chain or whatever can go through it. This item comes in a variety of sizes. When asked before everyone said its called a Bail. Well the Bails I've found are v shaped with prongs. Please if your...
by camaro
Mon Nov 10, 2003 10:44 am
Forum: Techniques and Tools
Topic: Melissa Paxton Bowls
Replies: 18
Views: 16395

Regarding Technique

I have been to Melissa's studio here in Texas, because I only live 30 min. from her studio. I know what she uses, however she is guarded over info involving her technique. As an artist and now a fuser, I'm curious as to why other artist feel threatened by others in the same field. No one can duplica...