Search found 1 match

by cheryl ~
Fri Apr 09, 2004 6:06 pm
Forum: Techniques and Tools
Topic: Need Your help with A Mold for A Paper Weight
Replies: 1
Views: 4610

check out UGOTGLASS at the top of the page--she tells you and shows you how to do it --I did it like she said and they came out great! one of the few things to turn out!!!!

have fun