Search found 2 matches

by DIHLEE
Mon Mar 01, 2004 5:31 pm
Forum: Techniques and Tools
Topic: A temperature for slump and fuse into sink mold
Replies: 7
Views: 13908

Thanks Bert, The size of the glass is 20" round 1/2"thick, two layer of float glass to slump and fuse into ( the same time) a metal mold for sink. My question is ? If I go to Temp. 1285 F the Thickness of the sink wall will be even still ? or I have to fuse two layer together first and slu...
by DIHLEE
Mon Mar 01, 2004 2:26 am
Forum: Techniques and Tools
Topic: A temperature for slump and fuse into sink mold
Replies: 7
Views: 13908

A temperature for slump and fuse into sink mold

hi all, I need to slump two layer of 1/2" Float glass into a sink mold (matel mold ) I have slumped sinks in the past using one layer 3/4" of Float glass @ Temperature of 1160 F. Is 1160 F an adequate max temperature to fuse and slump two layer of Float glass together properly into a sink ...