Cement/concrete mixer! 1, Remove any paint from inside the mixer. 2, Chop up a sheet of glass or use waste. 3, Throw glass in the mixer with a few heavy metal objects. 4, Cover the opening of the mixer to reduce dust. 5, Fit some extraction to the centre of the cover (optional but recommended) this ...
- Sun Mar 07, 2004 2:49 pm
- Forum: Techniques and Tools
- Topic: Tried and tested sand casting mold question
- Replies: 7
- Views: 8127
- Fri Mar 05, 2004 8:27 pm
- Forum: Techniques and Tools
- Topic: Tried and tested sand casting mold question
- Replies: 7
- Views: 8127
- Thu Mar 04, 2004 6:04 pm
- Forum: Techniques and Tools
- Topic: Tried and tested sand casting mold question
- Replies: 7
- Views: 8127
Tried and tested sand casting mold question
What is the best way to create a good re-usable mold for sand casting (crack free and smooth after drying) Or the most suitable way to repair any cracks / blemishes. I know there are several suggestions about additives to the sand but which one works the best?
Thankyou for your time.... XL
Thankyou for your time.... XL