Search found 2 matches

by Larry Cush
Sun May 04, 2003 10:42 pm
Forum: Techniques and Tools
Topic: Glastar Blaster Foot Pedal Problem
Replies: 6
Views: 13964

I have the same problem with my glastar foot pedal. I have found that it stops working properly when the pressure in my wimpy compressor cant keep up. I find I have to stop and shut off the mixing valve and air valve then empty the excess grit from the blast hose. I then restart the valve settings a...
by Larry Cush
Wed Mar 12, 2003 2:09 am
Forum: Techniques and Tools
Topic: wok trouble
Replies: 10
Views: 28920

I guess Im lucky, I just heat the wok on the stove and airbrush kilnwash on. It seems to stick fine and so far the glass hasnt stuck to it . I do get scaling on the back of the wok as it isnt stainless but it isnt coming thru the wash yet!
Larry