Search found 1514 matches

by Brad Walker
Wed Apr 08, 2026 2:14 pm
Forum: Techniques and Tools
Topic: Sunshine enamels
Replies: 3
Views: 4674

Re: Sunshine enamels

We store mixed up enamels in a small plastic jar. If you use A-14 as the binder, they can be stored for years.

Mixing instructions at the bottom of this page: https://warmglass.com/enamels/
by Brad Walker
Tue Mar 31, 2026 2:16 pm
Forum: Techniques and Tools
Topic: Kiln Shelf
Replies: 1
Views: 9382

Re: Kiln Shelf

I don't believe anyone makes an extruded ceramic/clay shelf that large anymore. Used to get them from Dyson, but they're no longer around. The biggest cordierite shelf I'm aware of is around 25" square. The best alternative is probably a fiber shelf, which is available in sizes that large. Won'...
by Brad Walker
Fri Mar 13, 2026 9:56 am
Forum: Newcomer Forum
Topic: Glass Kilns Causing Wireless Interference?
Replies: 2
Views: 70321

Re: Glass Kilns Causing Wireless Interference?

Never heard of this being a problem.

We have as many as 7 kilns running at the same time and have no trouble with our wireless network while they're on.
by Brad Walker
Tue Mar 03, 2026 10:49 pm
Forum: Techniques and Tools
Topic: toyo TB-19/600 thick glass cutter
Replies: 5
Views: 210793

Re: toyo TB-19/600 thick glass cutter

I believe the black cutter is still available, just not the rest of the system. I've used the cutter by itself before, works fairly well for straight cuts in glass up to around 1/2". The blade is at a different angle than the regular cutter. Are you trying to cut straight lines or curved ones? ...
by Brad Walker
Tue Nov 25, 2025 11:55 am
Forum: Techniques and Tools
Topic: rough surface on plate
Replies: 3
Views: 159010

Re: rough surface on plate

You'll need to give us more information.

What glass? What firing schedule? Got a photo?
by Brad Walker
Tue Sep 30, 2025 3:59 pm
Forum: Techniques and Tools
Topic: Tack fuse schedule for 14” cone art kiln
Replies: 4
Views: 120885

Re: Tack fuse schedule for 14” cone art kiln

DawnEllis59 wrote: Tue Sep 30, 2025 3:34 pm When you say watch the kiln can i carefully open the lid and peek in?
Yep. The key word is carefully. And just peek, don't hold it open very long.
by Brad Walker
Tue Sep 30, 2025 2:57 pm
Forum: Techniques and Tools
Topic: Tack fuse schedule for 14” cone art kiln
Replies: 4
Views: 120885

Re: Tack fuse schedule for 14” cone art kiln

The second kiln fires hotter than the first, so you'll need to reduce the top temperature (from 1325 to something less than that). Exact temperature depends on the particular kiln and degree of tack you want. Try 1300 and watch the kiln to see if that works. If not, go higher or lower than that to h...
by Brad Walker
Sat Sep 13, 2025 9:28 pm
Forum: Techniques and Tools
Topic: slump after sandblast?
Replies: 4
Views: 102920

Re: slump after sandblast?

I guess it depends on how low you can go and still achieve the slump you want. The lower the better, the shorter hold the better.

You could test with a scrap to see if you like the resulting texture.
by Brad Walker
Sat Sep 13, 2025 2:41 pm
Forum: Techniques and Tools
Topic: How thick a layer of powder?
Replies: 2
Views: 111875

Re: How thick a layer of powder?

The answer is going to depend on the color, but typically powder shrinks up to 1/2.

Why do you want the powder so thick? Can it work with a layer of thin (2mm) and a little less powder?
by Brad Walker
Sat Sep 13, 2025 2:39 pm
Forum: Techniques and Tools
Topic: slump after sandblast?
Replies: 4
Views: 102920

Re: slump after sandblast?

At 1250F most of the sandblasted surface will start to shine.

If you can, go to around 1125 and hold for an hour. That works for most shallow molds and will leave you a very nice matte surface. (My favorite finish, by the way.)
by Brad Walker
Thu Sep 04, 2025 10:03 pm
Forum: Techniques and Tools
Topic: Dealing with bubble in glass
Replies: 13
Views: 337948

Re: Dealing with bubble in glass

If I was trying to fix it though, you're saying put clear frit in the space of the bubble? Would that help the bubble flatten or would it just smooth out the the divot? If I wanted to keep working on the piece, I'd probably break the bubble and put frit or small pieces of glass where the bubble is....
by Brad Walker
Wed Sep 03, 2025 9:38 pm
Forum: Techniques and Tools
Topic: Dealing with bubble in glass
Replies: 13
Views: 337948

Re: Dealing with bubble in glass

I refired my second piece and ended up with a small bubble going the other direction and was wondering if anyone had any feedback. It's hard to tell without a better photo, but my guess is that when the original bubble happened it stretched the glass in that area and you didn't have enough thicknes...
by Brad Walker
Mon Aug 11, 2025 9:44 am
Forum: Techniques and Tools
Topic: Dealing with bubble in glass
Replies: 13
Views: 337948

Re: Dealing with bubble in glass

If I want the glass smoother, rather than more like a task fuse, how long do you recommend holding it at the top temp? Or is that more a matter of what the top temp is? The smartest thing to do is to keep the hold time the same and just vary the temperature. 10 minutes is a good standard to use. If...
by Brad Walker
Mon Aug 11, 2025 8:14 am
Forum: Techniques and Tools
Topic: Dealing with bubble in glass
Replies: 13
Views: 337948

Re: Dealing with bubble in glass

Also, when I refire, I was thinking of putting fiber paper on the bottomto help with airflow around the piece. Can I put kiln paper (I have Bullseye Thinfire) on top of the fiber paper to try and mitigate the rough texture or would that defeat the purpose of the fiber paper? Is fiber paper somethin...
by Brad Walker
Sun Aug 10, 2025 9:11 pm
Forum: Techniques and Tools
Topic: Dealing with bubble in glass
Replies: 13
Views: 337948

Re: Dealing with bubble in glass

Not long enough for a bubble hold. You need to hold at least 30 minutes at 1230F on the way up. Too fast from the bubble hold to your top temperature. 200 dph at the most. Too long a hold at the top temperature. Lots of lousy schedules at Makerspace and Reddit. As for refiring the damaged pieces, yo...
by Brad Walker
Wed Aug 06, 2025 9:19 pm
Forum: Techniques and Tools
Topic: Dealing with bubble in glass
Replies: 13
Views: 337948

Re: Dealing with bubble in glass

In general, it helps if you give us the firing schedule you used that caused the problem. The bubble was likely caused by firing too fast between 1200 and your top temperature. If you share your schedule we can answer more definitively. Slumping the piece won't fix the problem. And you can't fix it ...
by Brad Walker
Mon Jul 07, 2025 2:38 pm
Forum: Techniques and Tools
Topic: strong, but thin gloves?
Replies: 4
Views: 220603

Re: strong, but thin gloves?

We mostly use 5 mil, which might be easier than 9 mil to get on and off, but they're still hard to remove, especially if you're sweating.

Vinyl gloves would be easier to remove, but they're not very durable.
by Brad Walker
Mon Jul 07, 2025 10:28 am
Forum: Techniques and Tools
Topic: strong, but thin gloves?
Replies: 4
Views: 220603

Re: strong, but thin gloves?

Here are some options: Nitrile gloves, durable and resistant to puncture. Not quite as flexible as Latex surgical gloves, which are more prone to puncture than nitrile gloves. Vinyl gloves are thin, but prone to puncture Neoprene gloves are designed to replicate latex (some people are allergic to la...
by Brad Walker
Sun Jul 06, 2025 9:20 am
Forum: Techniques and Tools
Topic: Using raw oxides to color glass
Replies: 4
Views: 156307

Re: Using raw oxides to color glass

See here for a little more info: https://warmglass.com/phpBB3/viewtopic.php?p=364187 There's a nice chart about half way down the thread Most of the Ferro frits are no longer being made, but you might try some of these: https://ceramicsupplyusa.com/product-category/frits/ Or perhaps a local pottery ...
by Brad Walker
Wed Jun 11, 2025 2:58 pm
Forum: Techniques and Tools
Topic: No Days glass fusing glue
Replies: 3
Views: 144253

Re: No Days glass fusing glue

You might ask the No Days people: https://nodaysadhesives.com/No-Days-Liq ... g-c5749935

Don't know if it will work for you, but hot glue is polymer based so shouldn't be water soluble. It burns off pretty clean, but you may want to test for your application if you try it.