Use a little soap with stainless steel shot. Be sure to keep the load clean as the silver will be burnishing in dirty water if not clean . If the silver is textured you will get a great polish with ss shot and soapy clean water . If large & very flat will not be as good as Polish. If small and f...
by Lou_Ohio
Tue Dec 23, 2003 6:12 pm
Forum: Techniques and Tools
Topic: Granite Irid
Replies: 12
Views: 20952

I use this glass alot ... irid surface on the smooth side .
Will lose the texture on all glass at fusing tempertures .
Will usually lose the Irid surface at fusing temperture on Spectrum Glass.
Try System 96 or Bullseye to keep Irid surface).
Lou
by Lou_Ohio
Sat Dec 13, 2003 2:56 pm
Forum: Photos and Stuff
Topic: Menorah sharing time
Replies: 8
Views: 16414

try this reference itty bitty candle cup holders Robin Z <zeeski@worldnet.att.net> -- Monday, 18 February 2002 at 16:46 Licha & Jackie I found the Phone # 1-800-645-7260 & the Idem # 2815 Brass candle socket. Hope its what you want. Robin Z NEW: Re: itty bitty candle cup holders Jackie Beckm...
by Lou_Ohio
Tue Dec 09, 2003 10:04 pm
Forum: Techniques and Tools
Topic: The return of the glue test...
Replies: 9
Views: 16764

I have also had an intermitted problem with white glues (including emlers). I use super glue mostly. After a tight assembly , without glue, I place a small drop of super glue at many of the intersection (not all). The super glue burns off completely , is fast setting but if a lot is used it does sme...
by Lou_Ohio
Mon Dec 08, 2003 10:42 pm
Forum: Techniques and Tools
Topic: Glue Experiment
Replies: 4
Views: 8484

super glue.
what happen to the pic ?
by Lou_Ohio
Mon Dec 08, 2003 10:34 pm
Forum: Business Topics
Topic: Begging letter
Replies: 7
Views: 14055

I am from Cleveland and have no idea what the MS stands for (just BS).
Saw your work at the JCC last year … great stuff.
by Lou_Ohio
Sun Aug 24, 2003 12:57 pm
Forum: Techniques and Tools
Topic: Fine Silver and BE White
Replies: 2
Views: 6200

I have used this combination ( opal white & Fine silver ) without a problem .

Lou
by Lou_Ohio
Sat Apr 26, 2003 11:04 am
Forum: Business Topics
Topic: Jewelry Findings Suppliers
Replies: 10
Views: 32357

Geri Saw your post about mokemegame. I also have been cured of the need to make this material . After actually making it ( with a Power Break rolling Mill) and then using it some jewelry design ... no one cared . Could not sell it . I think it takes a lot education to a client to understand what it ...