- Mon Mar 31, 2003 12:22 am
- Forum: Techniques and Tools
- Topic: Glass cutters
- Replies: 15
- Views: 17952
Re: cutter and small hands
[/quote] The only thing I didn't like about the custom grip cutter is the handle swivels around and isn't tight on the body of the cutter. Everytime I picked the cutter up it took two hands to get the thing lined up, so I wrapped some heavy thread between the body and the handle and that keeps the a...
- Fri Mar 28, 2003 2:48 pm
- Forum: Techniques and Tools
- Topic: Glass cutters
- Replies: 15
- Views: 17952
I'm kind of interested in getting Toyo pistol grip since I've heard great things about them, but my concern is that you can't see what you are cutting. When I cut I bend my knees just a little and watch the line I've drawn on the glass while I'm cutting as I cut from away from me toward me (does th...
- Fri Mar 28, 2003 12:54 pm
- Forum: Techniques and Tools
- Topic: Glass cutters
- Replies: 15
- Views: 17952
- Fri Mar 28, 2003 10:28 am
- Forum: Techniques and Tools
- Topic: glass table tops and safety concerns...
- Replies: 20
- Views: 32882
works both ways
Interesting story about the public's perception of glass...I was recently told that I made the short list of artists for a large public art commission and that the committee loved my work and my concept. I proposed medium-sized cast glass pieces that would be siliconed in a metal framework. However...
- Fri Mar 28, 2003 10:23 am
- Forum: Techniques and Tools
- Topic: Glass cutters
- Replies: 15
- Views: 17952
- Fri Mar 28, 2003 1:30 am
- Forum: Techniques and Tools
- Topic: Glass cutters
- Replies: 15
- Views: 17952
Re: Glass cutters
I need to buy a new glass cutter, and have been considering a Toyo. Does anyone know what "tap" designates in the Toyo Tap Wheel Supercutter. I haven't been cutting glass for very long, and I don't know how the Tap Cutter is different from the regular Toyo cutter other than the ergonomic ...
- Thu Mar 27, 2003 9:59 am
- Forum: Techniques and Tools
- Topic: OK, new Felesatti grinder questions
- Replies: 7
- Views: 9659
Flex grinder
I just got a sale flyer from Gran Quartz. They have a limited number of Flex LW 1503 wet grinders, reconditioned for $199, it has a built in GFCI and water feed hookup.
Alpha Ceramica polishing disks run from $24.8 (3") to 48.4 (5") for resin discs from 150 - 3000 grit.
Alpha Ceramica polishing disks run from $24.8 (3") to 48.4 (5") for resin discs from 150 - 3000 grit.
- Wed Mar 26, 2003 9:28 pm
- Forum: Techniques and Tools
- Topic: Distance from top elements to glass?
- Replies: 7
- Views: 12112
Re: Distance from top elements to glass?
Sounds counter intuitive, especially given that Unifrax makes 10" thick Durablanket modules. Why would they do that if there was a problem with more than 6" of insulation? Probably irrelevant in this case anyway. Even if I used brick to fill up the kiln, I'd put a layer of blanket on top o...
- Wed Mar 26, 2003 1:29 pm
- Forum: Photos and Stuff
- Topic: Todays Pot Melt
- Replies: 37
- Views: 49683
links don't work
links don't work for me
- Wed Mar 26, 2003 1:26 pm
- Forum: Techniques and Tools
- Topic: silver fuming...
- Replies: 7
- Views: 10150
- Wed Mar 26, 2003 10:30 am
- Forum: Techniques and Tools
- Topic: silver fuming...
- Replies: 7
- Views: 10150
Re: silver fuming...
Okay, so I fired a bunch of tests in my kiln of silver leaf and its affect on different glass colors. I must have "fumed" my kiln shelf. Lazy girl didn't scrape and re-wash her shelf because a: the wash was intact b: she was only firing test tiles c: she is lazy d: all of the above And th...
- Tue Mar 25, 2003 12:06 pm
- Forum: Techniques and Tools
- Topic: slumping large pc
- Replies: 10
- Views: 13723
Robert, They are expecting it to look similar to when you drape a piece over a floral former, irregular and freeform....do you still think I should go slow? Thanks for your response, Sherry Sherry If you want it to wrinkle, I would go fast. Be sure to anneal slowly as sometimes the wrinkles touch a...
- Mon Mar 24, 2003 3:15 pm
- Forum: Techniques and Tools
- Topic: Hanging your Piece Question
- Replies: 6
- Views: 11294
Re: Hanging your Piece Question
I just made a Stained Glass panel that has a 2lb cast piece in the center. The panel is round (4 sq ft) framed in 1/2" came. I know when adding the rings to hang with, I need to run the wire into the seams for a stronger hold. Well the panel was hanging about 4 hours when I noticed the solder ...
- Mon Mar 24, 2003 3:03 pm
- Forum: Business Topics
- Topic: Another Insurance Question
- Replies: 8
- Views: 13788
- Mon Mar 24, 2003 3:01 pm
- Forum: Techniques and Tools
- Topic: glass table tops and safety concerns...
- Replies: 20
- Views: 32882
Re: glass table tops and safety concerns...
I have been making glass table tops. So far nothing larger than 20 inches. They are about 1/2 inch thick and set into, not ontop of the frames. My concern is safety. When I market these tops or tables must I include a layer of tempered glass to lay fused glass on top of or write a disclaimer or not...
- Mon Mar 24, 2003 10:28 am
- Forum: Business Topics
- Topic: Another Insurance Question
- Replies: 8
- Views: 13788
Re: Another Insurance Question
It sounds like there are a few of you that are still able to get business insurance. Is there anyone doing commissioned work that can give me the insurance carrier that they are using? I am in Colorado, and have been trying to get my business re-insured for the past year. I have run into one dead-e...
- Mon Mar 24, 2003 10:23 am
- Forum: Techniques and Tools
- Topic: Painters:Badger blender static?
- Replies: 10
- Views: 13295
I frequently wash my blender with soap and warm water. I take it no one else has encountered this so perhaps ambient dust, but it seems to happen after several smooth dust free blending strokes, then dust seems to appear. I have to tell you I feel laughed at here. Ha Ha. Not at all Joseph, nobody i...
- Mon Mar 24, 2003 10:22 am
- Forum: Techniques and Tools
- Topic: Painters:Badger blender static?
- Replies: 10
- Views: 13295
Not at all Joseph, nobody is laughing at you. I clean and dry my brushes the same way as Bert described. Then store them 'whiskers up' in a glass. The bristles have a paper 'hat' to keep them clean and dry. I try to keep the workplace, as when gilding, as clean and dust-free as possible. Paul Joe D...
- Sun Mar 23, 2003 11:50 pm
- Forum: Business Topics
- Topic: Shipping and Insurance Questions
- Replies: 15
- Views: 22794
- Sun Mar 23, 2003 11:45 pm
- Forum: Techniques and Tools
- Topic: Cheap glass
- Replies: 8
- Views: 10459