[You mean they don't call it eMpTy for nothing!]
Not for nothing. It's Big, it's Dry, it's very M.T.: 2-1/2 times the size of New England, with fewer people than New Hampshire (from whence I emigrated 13 years ago).
Pam[/quote]
Search found 14 matches
- Sun Oct 26, 2003 12:45 pm
- Forum: Techniques and Tools
- Topic: Help on making a ceramic seamless kiln shelf
- Replies: 10
- Views: 18525
- Sat Oct 25, 2003 12:11 am
- Forum: Techniques and Tools
- Topic: Help on making a ceramic seamless kiln shelf
- Replies: 10
- Views: 18525
- Fri Oct 24, 2003 8:58 am
- Forum: Techniques and Tools
- Topic: Help on making a ceramic seamless kiln shelf
- Replies: 10
- Views: 18525
Help on making a ceramic seamless kiln shelf
I have an Evenheat oval kiln (2541-13) with a 3-piece shelf and have been wondering if I could make a large seamless shelf using clay. I have tons of low-fire clay but I don't know if that would hold up to repeated firings. As we have a world-class ceramic facility in town (the Archie Bray) I can ac...
- Thu Oct 16, 2003 10:00 pm
- Forum: Business Topics
- Topic: waterproof my new canopy?
- Replies: 8
- Views: 18325
Buy some hula hoops. Wedge them between the canopy top and the metal scissor which connects the corners, with the majority of the hoop above the metal. They'll keep the top from acting like a collector and, if it isn't raining, provide you with something to do during those lulls in traffic. Pam ~~~~...
- Wed Oct 15, 2003 10:26 am
- Forum: Techniques and Tools
- Topic: E-6000 glue trouble for 1st time
- Replies: 19
- Views: 40129
- Tue Oct 14, 2003 7:29 pm
- Forum: Techniques and Tools
- Topic: Circle Cutter
- Replies: 17
- Views: 31290
I recently purchased one on ebay. It arrived with no cutting wheel in the cutter head. I emailed the seller several times but got no reply until I threatened to contact ebay and paypay and to leave bad feedback. Then I had to send digital photos of the bad head. Another 10 days (from CA to MT!-- the...
- Tue Oct 14, 2003 7:23 pm
- Forum: Techniques and Tools
- Topic: E-6000 glue trouble for 1st time
- Replies: 19
- Views: 40129
Very timely. I had a picture frame which was glued to a lucite stand develop a crack in both the lucite and the glass. E-6000. I've had this happen before with both mirrors and picture frames and attributed it to being knocked around although I wrap everything in bubble wrap whenever I move it. To s...
- Mon Aug 18, 2003 11:58 pm
- Forum: Techniques and Tools
- Topic: How do I make a 1-piece shelf from a 3-pc. shelf?
- Replies: 4
- Views: 8840
- Sat Aug 16, 2003 11:23 pm
- Forum: Techniques and Tools
- Topic: How do I make a 1-piece shelf from a 3-pc. shelf?
- Replies: 4
- Views: 8840
How do I make a 1-piece shelf from a 3-pc. shelf?
I have a new Evenheat 2542 kiln with a three-piece shelf and would like to be able to make something larger than what each individual piece can accommodate. What is the best way to span the gap between pieces? A single sheet of fiberboard?
Pam
Pam
- Tue Jul 29, 2003 12:09 pm
- Forum: Business Topics
- Topic: Concealing White Tent Walls
- Replies: 9
- Views: 15475
I didn't completely hide my walls, but I reduced them to background status. I picked up several yards of faux silk material (polyester; it feels like silk but doesn't wrinkle) in purple, turquoise blue and deep royal blue (wanted a green but they didn't have it). I cut 8' long pieces, hemmed the bot...
- Tue Jul 29, 2003 11:47 am
- Forum: Techniques and Tools
- Topic: Your Town, WA or OR
- Replies: 15
- Views: 24955
Your Town, WA or OR
Wanderlust is biting hard again. I've been in MT for 13 years and my feet are getting itchy. I'm thinking about relocating to NW OR or SW WA; ideally, I'd like to find a small, rural town where I can grow things (i.e., more than the 12" of precip. I get here, but 65" would probably make me...
- Sun Jul 27, 2003 12:37 am
- Forum: Techniques and Tools
- Topic: Circle-cutting miracle?
- Replies: 24
- Views: 37185
Re: Circle-cutting miracle?
there's nothing in physics about this. once the crack occurs, there's no surface tension left. it has to do with the fact that if the cut is completely vertical, there's no bevel on an edge to trap the circle in the square, so it can fall right out. the hard part is getting a vertical cut. Huh? no ...
- Wed Jul 16, 2003 11:42 pm
- Forum: Business Topics
- Topic: selling suggestion
- Replies: 19
- Views: 33970
- Sat Mar 15, 2003 11:39 am
- Forum: Business Topics
- Topic: So, how do you market your work?
- Replies: 10
- Views: 30888
I live in Montana, not the hotspot for glass that some parts of the country are. So, I sell at street fairs around the state where I can command fair prices and am going to try my first out-of-state show in August (if I get juried in). I tried a wholesale show in Seattle in January. I learned a few ...