Search found 18 matches

by ernest porcelli
Sat Jan 24, 2004 5:48 pm
Forum: Kiln Casting
Topic: Glass tile re productions need a caster
Replies: 2
Views: 7244

glass tiles

for those who need to know the web i was given is http://www.archituralglassinc.com
by ernest porcelli
Fri Jan 23, 2004 11:59 am
Forum: Kiln Casting
Topic: Glass tile re productions need a caster
Replies: 2
Views: 7244

Glass tile re productions need a caster

looking to re produce the FLW type glass tiles 3/8 " thick 4x4 tile we have samplesthey are 1/2 reed on one side 1/8 the other some have roundish bumps on them we need to make around 300 pieces for a landmark building NYC if interested please call 718-596-4353
by ernest porcelli
Fri Jan 23, 2004 11:47 am
Forum: Kiln Casting
Topic: looking for reproduction of glass tiles
Replies: 0
Views: 9598

looking for reproduction of glass tiles

have samples, need 300 pieces of glass, FLW type tiles 3/8 thick 4x4 1/2 reed one side 1/8 reed other some have bumps as well landmark building NYC, need price, lead time if interest please call 718 596 4353 thank you ernest
by ernest porcelli
Thu Jan 22, 2004 5:02 pm
Forum: Business Topics
Topic: Wholesalers
Replies: 9
Views: 19747

thank you all

it seems to me everyone points are important i sometimes pack $1300 into a box that cost me $7:50 plus the insurance etc so if i'm charging 5% it doesn't cover the time to pack or the material,i trying to make $$$ here,the 10% would work for me but it would be a big increase to start with, its now 8...
by ernest porcelli
Thu Jan 22, 2004 9:52 am
Forum: Business Topics
Topic: Wholesalers
Replies: 9
Views: 19747

Wholesalers

i'm interested to hear what others charge to ship works to stores selling your works. right now i charge 5% i'm not sure it's enought with the cost of insurance, packing material etc. thank you for your replys ep
by ernest porcelli
Tue Jan 13, 2004 5:41 pm
Forum: Business Topics
Topic: wholesale crafts.com, input?
Replies: 10
Views: 21981

wholesalecrafts .com

nice people to work with ,the thing i found about their site was you the artist have to work the site meaning you have to up date your photos frequently to be on the new works pages, i didn't have the time needed to work it, got not enough orders from them . had lots of inquires from the group ads, ...
by ernest porcelli
Tue Jan 13, 2004 9:09 am
Forum: Business Topics
Topic: Wholesale,Rosen
Replies: 3
Views: 7500

Wholesale,Rosen

any advise from those who have done the Rosen show in philly? What can a poor boy expect ? How much stuff do i put out? It's my first time there. Thanks to all who respond. ep
by ernest porcelli
Sat Jan 03, 2004 12:21 pm
Forum: Techniques and Tools
Topic: fused glass lampshade
Replies: 2
Views: 6195

hole

when you lay out the glass for fusing you could leave the space you need to wire the shade,anyway that is how i produce them,check my web site ep
by ernest porcelli
Mon Dec 22, 2003 10:25 am
Forum: Techniques and Tools
Topic: laminate fused glass to 3/16 plate
Replies: 4
Views: 9639

laminate fused glass to 3/16 plate

anyone know how to laminate a fused glass piece about 24"x24" to a piece of plate. this laminated piece is then to be drilled with 1" holes.if it works i need to make 6 panels. anyone ever do such a project? thank you for your help ep
by ernest porcelli
Mon Sep 29, 2003 9:11 am
Forum: Techniques and Tools
Topic: scotch tape' am i the only one
Replies: 20
Views: 42607

scotch tape' am i the only one

i've use this tape for years to hold pieces of glass together to get works from the bench to the kiln. yes you need to support the piece with the top glass or card board to move it into the kiln, the tape burns off i've even used the tape between both layers and not had any problems with the finshed...
by ernest porcelli
Thu Sep 25, 2003 5:20 pm
Forum: Business Topics
Topic: art show- carry-out, or deliver?
Replies: 18
Views: 38135

shipping

If you tell someone shipping IS available it may make the sale, just charge enough to cover your expeances, time and matieral. Buyers like options. a small sign i display in my booth shipping available it about selling have fun selling ep
by ernest porcelli
Tue Sep 23, 2003 11:45 am
Forum: Business Topics
Topic: Outside set ups.
Replies: 8
Views: 15454

Display

I use tables i got from Costco the 24 x48 add 8 inches with pipe and screws to make table high to 42". the pipe can be ajustable for uneven ground ,your out doors add risers for different hights ep
by ernest porcelli
Thu Apr 10, 2003 3:11 pm
Forum: Techniques and Tools
Topic: Warm Glass conference -- hotel poll
Replies: 14
Views: 29433

rooms

if u don' t do price line shame on u ep
by ernest porcelli
Mon Mar 31, 2003 5:50 pm
Forum: Techniques and Tools
Topic: Fusing & Glue
Replies: 6
Views: 15877

Glue?

i use elmer's for some projects, but what i found to work the best to get large pieces (25x25) into by kiln is scotch tape 3M majic tape. tape the glass on the bottom ,use fiber paper, almost all my works have clear top glass,so i use it(top glass) to slide the taped glass into the kiln , like it wa...
by ernest porcelli
Thu Mar 27, 2003 9:58 am
Forum: Techniques and Tools
Topic: hi-heart lead and fused glass
Replies: 15
Views: 29304

frame

tess if you have an iron shop around have them make a steel frame, drill holes , epsolder copper wire to the lead to hold the panel into the frame. you would have to finish the steel with paint to prevent rust. i like useing 1"angle,but i've used 1/2" as well
by ernest porcelli
Wed Mar 26, 2003 9:23 am
Forum: Techniques and Tools
Topic: hi-heart lead and fused glass
Replies: 15
Views: 29304

high heart

i use a 1/4 "normal lead from Bendheim&co, if the glass is to thick , grind as if it was ripple glass.the important thing is brass or tin fins for structural support . ep
by ernest porcelli
Mon Mar 24, 2003 6:41 pm
Forum: Techniques and Tools
Topic: Hanging your Piece Question
Replies: 6
Views: 18897

support

what would work is a steel frame ,3/4 angle and tin fins soldered on the back. lead would have been better to use for assembling. good luck with your competition ep
by ernest porcelli
Thu Mar 13, 2003 6:27 pm
Forum: Techniques and Tools
Topic: Need a studio that does slumped glass work in NJ/NY area
Replies: 2
Views: 11090

Flickinger Glass Works 718 875 1531 Brooklyn ny can slump your lamp panels ep