If you know a potter who uses a slab roller, have him make a slab and cut it into strips. If the slab is 1/2" thick you can slice them to the hieght you want to build your pattern bars. Care must be taken to keep them from twisting as they dry. I made mine by rolling the clay between two fixed ...