Re: fusing neon tubes

The neon tubing that I worked with in college (UW Madison) was all lead based glass. I'm not sure of the exact COE, but you could gather from the hot glass tank (96 COE) and use the neon tube as a blow pipe and make a little sculpture that would anneal down fine. The clear scrap made a nice kiln cas...