Search found 10 matches
- Fri Mar 19, 2004 2:47 pm
- Forum: Kiln Casting
- Topic: Kaiser Lee Board where to buy??/
- Replies: 4
- Views: 7259
Kaiser Lee Board where to buy??/
I read with interest the discussion on using what sound great -Kaiser Lee Board. I went to the website given but was unable to email, it was like a link but not email address. Thanks for the help. Pam
- Fri Mar 05, 2004 11:47 am
- Forum: Techniques and Tools
- Topic: Help! Moving to MAINE
- Replies: 17
- Views: 18684
- Tue Apr 15, 2003 7:05 am
- Forum: Techniques and Tools
- Topic: bubble problems
- Replies: 8
- Views: 8829
:lol: Good new,at least it looks that way. Thank-you all for your advise. I popped the bubble by scoring it and soing a little tapping. Refired very, very slow, and this morning before leaving for school I took a peek. The area where the big bubble was looks fine, at least for now, kiln at 700. Gues...
- Mon Apr 14, 2003 2:16 pm
- Forum: Techniques and Tools
- Topic: bubble problems
- Replies: 8
- Views: 8829
- Mon Apr 14, 2003 11:16 am
- Forum: Techniques and Tools
- Topic: bubble problems
- Replies: 8
- Views: 8829
bubble problems
Another problem with my beautiful blue/purple opal glass. I fused the broken cirlcle with cut out pieces of a large Kokopelli playing his flute to a dicro. moon. I filled in the broken line with frit. Well, it worked but needed to fill in one small point. I got the great idea to cap this baby with c...
- Mon Apr 14, 2003 10:36 am
- Forum: Techniques and Tools
- Topic: bubble problems
- Replies: 0
- Views: 21259
bubble problems
Another problem with my beautiful blue/purple opal glass. I fused the broken cirlcle with cut out pieces of a large Kokopelli playing his flute to a dicro. moon. I filled in the broken line with frit. Well, it worked but needed to fill in one small point. I got the great idea to cap this baby with c...
- Sat Apr 12, 2003 1:24 pm
- Forum: Techniques and Tools
- Topic: Where on the EAST coast to buy Bullseye and supplies?
- Replies: 8
- Views: 10662
- Fri Apr 11, 2003 2:51 pm
- Forum: Techniques and Tools
- Topic: Cutting BE Blue Opal, Plum 2100 series..help please
- Replies: 1
- Views: 3740
- Fri Apr 11, 2003 2:49 pm
- Forum: Techniques and Tools
- Topic: Cutting BE Blue Opal, Plum 2100 series..help please
- Replies: 1
- Views: 3740
Cutting BE Blue Opal, Plum 2100 series..help please
I'm trying to cut the BE opal glass, 2100 series, into a circle. I used my trusty circle cutter and did the tap, tap, tap, and not results. This glass did not seem to run along the score, and did not want to break. SO my one circle ended up in 3 pieces. I don't want to ruin the whol beautiful sheet ...
- Mon Mar 31, 2003 8:00 am
- Forum: Photos and Stuff
- Topic: Todays Pot Melt
- Replies: 37
- Views: 49192
pot melt 1st try
Randy, this is my first post on the new board, so hope this works ? I tried your pot melt last nite. I didn't hold it long enought so it was not finished dripping, I flashed cooled it and cracked the glass, and learned lots. I didn't know that the glass would react like paint at that high a temp. ie...