Search found 3 matches

by Kathleen Haydon
Fri Jul 12, 2013 10:20 pm
Forum: Newcomer Forum
Topic: How to add time during firing?
Replies: 2
Views: 7850

Re: How to add time during firing?

Thank you Brad
by Kathleen Haydon
Fri Jul 12, 2013 6:40 pm
Forum: Photos and Stuff
Topic: Colour Bars and Deep Slump
Replies: 14
Views: 32063

Re: Colour Bars and Deep Slump

Beautiful!
by Kathleen Haydon
Fri Jul 12, 2013 6:32 pm
Forum: Newcomer Forum
Topic: How to add time during firing?
Replies: 2
Views: 7850

How to add time during firing?

I have a rampmaster II and I would like to add additional annealing time. Is there a way to do this during the fire? The only thing I see in the manual is to push the pause button and temp. Should hold the same for an additional 30 min. Is this correct?